Novel composite proton-exchange membrane based on silica-anchored sulfonic acid (SASA)

被引:15
作者
Duvdevani, T.
Philosoph, M.
Rakhman, M.
Golodnitsky, D.
Peled, E. [1 ]
机构
[1] Tel Aviv Univ, Sch Chem, IL-69978 Tel Aviv, Israel
[2] Tel Aviv Univ, Wolfson Appl Mat Res Ctr, IL-69978 Tel Aviv, Israel
[3] Israel Plast & Rubber Ctr, Haifa, Israel
关键词
PCM; SASA; fuel cell; membrane; methanol oxidation;
D O I
10.1016/j.jpowsour.2006.06.006
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A new approach to the synthesis of a low-cost proton-exchange composite membrane (C-PEM) based on PVDF and silica with surface-anchored sulfonic acid (SASA) groups, is presented for the first time. SASA membranes of different compositions have been prepared and characterized with the use of SEM, DSC, TGA, BET and electrochemical techniques. The room-temperature conductivity of SASA-based C-PEMs, is in the range of 2.0-50 mS cm(-1). The equivalent weight of two SASA powders, SASA3(A) and SASA4(A) are 1600 and 2500 g equiv.(-1) respectively. The typical pore size as measured by BET is about 4 nm. The membrane is thermally stable up to 250 degrees C. Direct methanol fuel cells (DMFCs) have been assembled with some of the membranes. Preliminary tests show that the cell resistance with a non-optimized membrane is in the range of 3 Omega cm(-2), therefore the maximum cell power density achieved so far does not exceed 32 mW cm(-2) at 70 degrees C. The crossover-current density for a 100 mu m-thick membrane DMFC measured in 1 M methanol at 80 degrees C is 110 mA cm(-2) (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:1069 / 1075
页数:7
相关论文
共 21 条
[11]  
NARAYANAN SR, 1995, ELECTROCHEMICAL SOC, P261
[12]  
Peled E, 1998, ELECTROCHEM SOLID ST, V1, P210, DOI 10.1149/1.1390687
[13]   A direct methanol fuel cell based on a novel low-cost nanoporous proton-conducting membrane [J].
Peled, E ;
Duvdevani, T ;
Aharon, A ;
Melman, A .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2000, 3 (12) :525-528
[14]   High-power direct ethylene glycol fuel cell (DEGFC) based on nanoporous proton-conducting membrane (NP-PCM) [J].
Peled, E ;
Livshits, V ;
Duvdevani, T .
JOURNAL OF POWER SOURCES, 2002, 106 (1-2) :245-248
[15]   New fuels as alternatives to methanol for direct oxidation fuel cells [J].
Peled, E ;
Duvdevani, T ;
Aharon, A ;
Melman, A .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2001, 4 (04) :A38-A41
[16]  
PELED E, 2005, BATTERY 2005 PARIS E
[17]  
PELED E, 2004, ISPE 9 P MRAG POL
[18]  
REN X, 1996, J ELECTROCHEM SOC, V143
[19]   Solid polymer electrolyte membranes for fuel cell applications - a review [J].
Smitha, B ;
Sridhar, S ;
Khan, AA .
JOURNAL OF MEMBRANE SCIENCE, 2005, 259 (1-2) :10-26
[20]  
WARTHESEN SJ, 1999, 3 INT S NEW MAT EL S, P69