Effect of electrolytic hydrogen pre-charging on the cavitation erosion resistance of NiTi: a preliminary study

被引:16
作者
Cheng, FT [1 ]
Shi, P
Man, HC
机构
[1] Hong Kong Polytech Univ, Dept Appl Phys, Kowloon, Hong Kong, Peoples R China
[2] Liaoning Inst Technol, Dept Chem & Mat Engn, Liaoning 121001, Peoples R China
[3] Hong Kong Polytech Univ, Dept Mfg Engn, Kowloon, Hong Kong, Peoples R China
关键词
cavitation erosion; hydrogen charging; hydride; NiTi;
D O I
10.1016/S1359-6462(02)00099-4
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Specimens of a Ni-rich NiTi alloy was electrolytically pre-charged with hydrogen over a wide range of current densities (0.0001-0.1 A/cm(2)). The cavitation erosion resistance of all the hydrogen-charged specimens were significantly reduced. The decrease in resistance was attributed to the formation of hydride at the grain boundaries. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:89 / 94
页数:6
相关论文
共 24 条
[11]   Ordered intermetallic alloys: an assessment [J].
Liu, CT ;
Stringer, J ;
Mundy, JN ;
Horton, LL ;
Angelini, P .
INTERMETALLICS, 1997, 5 (08) :579-596
[12]  
MIYAHARA K, 1994, P C STRENGTH MAT ICS, P945
[13]   CRYSTAL-STRUCTURE OF A HYDRIDE FORMED BY ELECTROCHEMICAL HYDROGENATION IN A TI-NI-AL ALLOY [J].
NAM, TH ;
SHIMIZU, K ;
SABURI, T ;
NENNO, S .
MATERIALS TRANSACTIONS JIM, 1989, 30 (08) :539-548
[14]   ENVIRONMENTAL EMBRITTLEMENT IN L12-ORDERED (CO, FE)3V ALLOYS [J].
NISHIMURA, C ;
LIU, CT .
ACTA METALLURGICA ET MATERIALIA, 1992, 40 (04) :723-731
[15]  
Otsuka K., 1988, SHAPE MEMORY MAT
[16]  
Pelton B. L., 1997, SMST 97, P395
[17]   CAVITATION EROSION OF 2 NITI ALLOYS [J].
RICHMAN, RH ;
RAO, AS ;
HODGSON, DE .
WEAR, 1992, 157 (02) :401-407
[18]   WATER JET EROSION BEHAVIOR OF TI-NI BINARY-ALLOYS [J].
SHIDA, Y ;
SUGIMOTO, Y .
WEAR, 1991, 146 (02) :219-228
[19]   STRUCTURAL STUDY OF THE HYDRIDES NITIHX (X=1.0 AND 1.4) [J].
SOUBEYROUX, JL ;
FRUCHART, D ;
LORTHIOIR, G ;
OCHIN, P ;
COLIN, D .
JOURNAL OF ALLOYS AND COMPOUNDS, 1993, 196 (1-2) :127-132
[20]  
TAKASUGI T, 1996, INTERMETALLICS, V4, P5181