Effect of pressure difference on the quality of titanium casting

被引:72
作者
Watanabe, I [1 ]
Watkins, JH [1 ]
Nakajima, H [1 ]
Atsuta, M [1 ]
Okabe, T [1 ]
机构
[1] NAGASAKI UNIV,SCH DENT,DEPT FIXED PROSTHODONT,NAGASAKI 852,JAPAN
关键词
titanium; casting pressure difference; mechanical properties; porosity;
D O I
10.1177/00220345970760031001
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
In casting titanium using a two-compartment casting machine, Hero et al. (1993) reported that the pressure difference between the melting chamber and the mold chamber affected the soundness of the casting. This study tested the hypothesis that differences in pressure produce castings With various amounts of porosity and different mechanical properties values. Plastic dumbbell-shaped patterns were invested with an alumina-based, phosphate-bonded investment material. Both chambers of the casting machine were evacuated to 6 x 10(-2) torr; the argon pressure difference was then adjusted to either 50, 150, 300, or 450 torr. The porosity of the cast specimens was determined by x-ray radiography and quantitative image analysis. Tensile strength and elongation were measured by means of a universal testing machine at a strain rate of 1.7 x 10(-4)/s. The fractured surfaces were examined by SEM. Changes in Vickers hardness with depth from the cast surface were measured on polished cross-sections of the specimens. Raising the argon pressure difference to 300 and 450 torr caused a significant increase in internal porosity and a resultant decrease in the engineering tensile strength and elongation. The highest tensile strength (similar to 540 MPa), elongation (similar to 10%), bulk hardness (HV50g 209), and lowest porosity level(similar to 0.8%) occurred in the specimens cast at 150 torr. Turbulence of the metal during casting was thought to be responsible for the increase in porosity levels with the increase in argon pressure difference. By choosing an argon pressure difference (around 150 torr) suitable for this geometry, we could produce castings which have adequate mechanical properties and low porosity levels.
引用
收藏
页码:773 / 779
页数:7
相关论文
共 33 条
[1]   CLINICAL-RESULTS WITH TITANIUM CROWNS FABRICATED WITH MACHINE DUPLICATION AND SPARK EROSION [J].
ANDERSSON, M ;
BERGMAN, B ;
BESSING, C ;
ERICSON, G ;
LUNDQUIST, P ;
NILSON, H .
ACTA ODONTOLOGICA SCANDINAVICA, 1989, 47 (05) :279-286
[2]  
[Anonymous], 1986, MECH METALLURGY
[3]   A 2-YEAR FOLLOW-UP-STUDY OF TITANIUM CROWNS [J].
BERGMAN, B ;
BESSING, C ;
ERICSON, G ;
LUNDQUIST, P ;
NILSON, H ;
ANDERSSON, M .
ACTA ODONTOLOGICA SCANDINAVICA, 1990, 48 (02) :113-117
[4]  
BOYER R, 1994, TITANIUM ALLOYS MAT, P1057
[5]   POROSITY AND ACCURACY OF MULTIPLE-UNIT TITANIUM CASTINGS [J].
CHAI, TI ;
STEIN, RS .
JOURNAL OF PROSTHETIC DENTISTRY, 1995, 73 (06) :534-541
[6]  
CRAIG RD, 1993, RESTORATIVE DENT MAT, P421
[7]  
Etchu Y, 1987, Tohoku Shika Daigaku Gakkai Shi, V14, P130
[8]   DENTAL CASTING OF TITANIUM AND NI-TI ALLOYS BY A NEW CASTING MACHINE [J].
HAMANAKA, H ;
DOI, H ;
YONEYAMA, T ;
OKUNO, O .
JOURNAL OF DENTAL RESEARCH, 1989, 68 (11) :1529-1533
[9]   MOLD FILLING AND POROSITY IN CASTINGS OF TITANIUM [J].
HERO, H ;
SYVERUD, M ;
WAARLI, M .
DENTAL MATERIALS, 1993, 9 (01) :15-18
[10]  
Ida K, 1985, Dent Mater J, V4, P191