Effects of strain-rate and ageing at 573 and 973 K on the mechanical (compressive) behaviour of <110> oriented ('soft') NiAl single crystals with and without microalloying additions of Ti, Zr, and Hf .2.

被引:7
作者
Golberg, D [1 ]
Sauthoff, G [1 ]
机构
[1] MAX PLANCK INST EISENFORSCH GMBH, D-40074 DUSSELDORF, GERMANY
关键词
nickel aluminides; based on NiAl; microalloying; single crystal properties; strain-ageing; ductility; TRANSIENT FLOW BEHAVIOR; ALLOYS; DUCTILITY; TENSILE;
D O I
10.1016/0966-9795(95)00047-X
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of impurity gettering on the mechanical behaviour of NiAl have received extensive attention recently. The present work was directed at static and dynamic strain ageing phenomena and strain-rate sensitivity minima, which are supposed to be related to the dislocation-impurity interactions, for <110> oriented NiAl single crystals with microalloying additions of Ti, Hf and Zr as getters (0.1 at.%). The influence of ageing at 573 and at 973 K on compressive properties and microhardness was also investigated. The gettering effects were found to be less pronounced for NIAl + Ti and more pronounced for NIAl + H+ and NIAl + Zr, and the gettering effects lead to marked changes in the strength and ductility behaviour after ageing at 973 K as well as static strain-ageing at 573 K, and to strain-rate sensitivity. The observed effects are believed to be due to the formation of precipitates containing Ti, Hf, or Zr, their coarsening during ageing, and interactions of dislocations with either precipitates and/or solute atoms and interstitials. (C) 1996 Elsevier Science Ltd.
引用
收藏
页码:253 / 271
页数:19
相关论文
共 49 条
[31]   THEORY OF FLOW LOCALIZATION DUE TO DYNAMIC STRAIN AGING [J].
MCCORMICK, PG .
ACTA METALLURGICA, 1988, 36 (12) :3061-3067
[32]   EFFECT OF PRECIPITATION HARDENING ON DYNAMIC STRAIN AGING AND JERKY FLOW [J].
MULFORD, RA .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (10) :1527-1532
[33]  
MUNZ D, 1966, Z METALLKD, V57, P442
[34]  
NOEBE RD, 1993, INT MATER REV, V38, P193, DOI 10.1179/095066093790326276
[35]  
Pascoe R T., 1968, Metal Science, V2, P138
[36]   DEFORMATION MODES OF INTERMEDIATE PHASE NIAL [J].
PASCOE, RT ;
NEWEY, CWA .
PHYSICA STATUS SOLIDI, 1968, 29 (01) :357-&
[37]  
PAUFLER P, 1975, KRISTALLOGRAPHISCHE, P104
[38]   OBSERVATIONS ON THE BRITTLE TO DUCTILE TRANSITION-TEMPERATURES OF B2 NICKEL ALUMINIDES WITH AND WITHOUT ZIRCONIUM [J].
RAJ, SV ;
NOEBE, RD ;
BOWMAN, R .
SCRIPTA METALLURGICA, 1989, 23 (12) :2049-2054
[39]  
ROZNER AG, 1966, J I MET, V94, P169
[40]  
SINGLETON MF, 1986, BINARY ALLOY PHASE D, P140