Durability of poly(dimethylsiloxane) when exposed to chlorine gas

被引:11
作者
Eikeland, MS
Hägg, MB [1 ]
Brook, MA
Ottoy, M
Lindbråthen, A
机构
[1] Norwegian Univ Sci & Technol, Fac Chem Engn, N-7491 Trondheim, Norway
[2] Telemark Technol Res & Dev Ctr, N-3918 Porsgrunn, Norway
[3] McMaster Univ, Dept Chem, Hamilton, ON, Canada
关键词
poly(dimethylsiloxane); chlorine; degradation; permeability; absorption; Fourier transform infrared;
D O I
10.1002/app.10878
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Highly crosslinked poly(dimethylsiloxane) (PDMS) is discussed as an alternative membrane material for the gas separation of highly concentrated chlorine gas (90-95 vol %) and oxygen, due to an initial high permeation for Cl-2 and a high selectivity of Cl-2/O-2. It was found that the separation properties of the PDMS membrane change over time upon exposure to aggressive chlorine gas; the flux will go down, and the material may even degrade if not appropriately prepared and protected. The PDMS was exposed to chlorine gas over 4 weeks in a glass chamber at both 30 and 60degreesC and analysed by (FTIR). The membranes were exposed to chlorine gas in a permeation cell with measurements of the permeability of N-2, O-2, and Cl-2 at regular intervals. The temperature range for the permeation measurements was 30-100degreesC, and the pressure difference over the membrane was ca. 2 bar. The time of exposure in the permeation cell was several weeks. The absorption of N-2, O-2, and Cl-2 in the PDMS at temperatures in the same range was also measured. This article discusses the durability of the highly crosslinked PDMS membrane following chlorine exposure. (C) 2002 Wiley Periodicals, Inc.