Defect location of individual single-walled carbon nanotubes with a thermal oxidation strategy

被引:35
作者
Li, QW [1 ]
Yan, H [1 ]
Ye, YC [1 ]
Zhang, J [1 ]
Liu, ZF [1 ]
机构
[1] Peking Univ, Coll Chem & Mol Engn, Ctr Nanoscale Sci & Technol, Beijing 100871, Peoples R China
关键词
D O I
10.1021/jp026512c
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, we proposed a simple method to locate defect sites in individual SWNTs with an AFM technique by using a thermal oxidation strategy. After thermal oxidation of well-dispersed SWNTs on a silicon surface in air at 500 degreesC, almost all of the original SWNTs were fractured into short fragments. The range of the fragment sizes was different and closely related to the length and growth time of the tubes. The rupture of SWNTs was confirmed to be a result of the presence of defects in tubes and to be caused by the attack of oxygen molecules in air. Owing to the damage event that occurred in SWNTs after heating treatment, a thermal oxidation method may be developed as a potentially useful technique for the cutting of SWNTs, and chemical functionality of the SWNTs could also be achieved during this process. In this regard, a thermal treatment method would be employed as another useful cutting and functionalizing approach to tailor the chemical and physical properties of SWNTs.
引用
收藏
页码:11085 / 11088
页数:4
相关论文
共 24 条
[11]  
Fan YW, 2002, ADV MATER, V14, P130, DOI 10.1002/1521-4095(20020116)14:2<130::AID-ADMA130>3.0.CO
[12]  
2-Z
[13]  
HARMON MA, 2001, CHEM PHYS LETT, V347, P8
[14]   Structural modification of single-layer carbon nanotubes with an electron beam [J].
Kiang, CH ;
Goddard, WA ;
Beyers, R ;
Bethune, DS .
JOURNAL OF PHYSICAL CHEMISTRY, 1996, 100 (09) :3749-3752
[15]   Thermal degradation of ragged single-wall carbon nanotubes produced by polymer-assisted ultrasonication [J].
Koshio, A ;
Yudasaka, M ;
Iijima, S .
CHEMICAL PHYSICS LETTERS, 2001, 341 (5-6) :461-466
[16]   A scalable CVD synthesis of high-purity single-walled carbon nanotubes with porous MgO as support material [J].
Li, QW ;
Yan, H ;
Cheng, Y ;
Zhang, J ;
Liu, ZF .
JOURNAL OF MATERIALS CHEMISTRY, 2002, 12 (04) :1179-1183
[17]  
LIBER CM, 2001, SCIENCE, V291, P283
[18]   Fullerene pipes [J].
Liu, J ;
Rinzler, AG ;
Dai, HJ ;
Hafner, JH ;
Bradley, RK ;
Boul, PJ ;
Lu, A ;
Iverson, T ;
Shelimov, K ;
Huffman, CB ;
Rodriguez-Macias, F ;
Shon, YS ;
Lee, TR ;
Colbert, DT ;
Smalley, RE .
SCIENCE, 1998, 280 (5367) :1253-1256
[19]  
Louie SG, 2001, TOP APPL PHYS, V80, P113
[20]   Surface defect site density on single walled carbon nanotubes by titration [J].
Mawhinney, DB ;
Naumenko, V ;
Kuznetsova, A ;
Yates, JT ;
Liu, J ;
Smalley, RE .
CHEMICAL PHYSICS LETTERS, 2000, 324 (1-3) :213-216