共 21 条
High catalytic activity of pitch based activated carbon fibres of moderate surface area for oxidation of NO to NO2 at room temperature
被引:119
作者:
Mochida, I
[1
]
Kawabuchi, Y
[1
]
Kawano, S
[1
]
Matsumura, Y
[1
]
Yoshikawa, M
[1
]
机构:
[1] OSAKA GAS CO LTD,CTR RES & DEV,KONOHANA KU,OSAKA 554,JAPAN
来源:
关键词:
nitric oxide oxidation;
activated carbon;
pitch-based fibres;
D O I:
10.1016/S0016-2361(96)00223-2
中图分类号:
TE [石油、天然气工业];
TK [能源与动力工程];
学科分类号:
0807 ;
0820 ;
摘要:
Catalytic oxidation of NO (380 ppmv) to NO2 over activated carbon fibres of moderate surface area (similar to 800 m(2) g(-1)) at room temperature was carried out, to develop oxidative removal of NO from flue gas. The heat treatment of pitch-based activated carbon fibres of moderate surface area markedly increased the conversion of NO to 87% in dry air, 62% in air of 80% relative humidity and 24% in wet air (100% r.h.) at 25 degrees C and a ratio of fibre mass to gas flow rate of 1.0 x 10(-2) g min mL(-1). The strong inhibiting effect of humidity on the activity of the as-received fibres was moderated by heat treatment of the fibres at 850 degrees C. A lower concentration of 10 ppmv NO markedly reduced the oxidation, the conversions being 24 and 5% in dry and wet (100% r.h.) air respectively. The catalytic activities of other pitch-based fibres of different surface area were also much inferior in moist air above 60% r.h. (C) 1997 Elsevier Science Ltd.
引用
收藏
页码:543 / 548
页数:6
相关论文