Superparamagnetic zinc ferrite spinel-graphene nanostructures for fast wastewater purification
被引:208
作者:
Meidanchi, Alireza
[1
,2
]
Akhavan, Omid
[1
,3
]
机构:
[1] Sharif Univ Technol, Dept Phys, Tehran, Iran
[2] Payame Noor Univ, Dept Phys, Tehran, Iran
[3] Sharif Univ Technol, Inst Nanosci & Nanotechnol, Tehran, Iran
来源:
关键词:
NEURAL STEM-CELLS;
AQUEOUS-SOLUTION;
PHOTOCATALYTIC ACTIVITY;
CARBON NANOTUBES;
HIGH-PERFORMANCE;
FACILE SYNTHESIS;
OXIDE;
DIFFERENTIATION;
REDUCTION;
REMOVAL;
D O I:
10.1016/j.carbon.2013.12.019
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
Superparamagnetic ZnFe2O4/reduced graphene oxide (rGO) composites containing ZnFe2O4 nanoparticles (with similar to 5-20 nm sizes) attached onto rGO sheets (with similar to 1 mu m lateral dimensions) were synthesized by hydrothermal reaction method. By increasing the graphene content of the composite from 0 to 40 wt%, the size as well as the number of the ZnFe2O4 nanoparticles decreased and the saturated magnetization of the composites reduced from 10.2 to 1.8 emu/g, resulting in lower responses to external magnetic fields. Concerning this, the time needed for 90% separation of ZnFe2O4/rGO (40 wt%) composite from its solution (2 mg/mL in ethanol) was found 60 min in the presence of an external magnetic field (similar to 1 Tesla), while using ZnFe2O4/rGO (15 wt%), only 2 mm was required (comparable to the separation time of pure ZnFe2O4 nanoparticles). Correspondingly, the magnetic separation time of 10 pM methyl orange and rhodamine B from aqueous solutions containing 2 mg/mL ZnFe2O4/rGO (15 wt%) was found <6 min, while using the ZnFe2O4/rGO (40 wt%) only 15-20% of the dyes could be separated after 16 mm. Although the pure ZnFe2O4 nanoparticles could magnetically separate nearly whole of the dyes from the solutions, the separation time was too longer (>16 min). (C) 2013 Elsevier Ltd. All rights reserved.