Thermal Decomposition Approach for the Formation of α-Fe2O3 Mesoporous Photoanodes and an α-Fe2O3/CoO Hybrid Structure for Enhanced Water Oxidation
被引:32
作者:
Diab, Mahmud
Mokari, Taleb
[1
]
机构:
[1] Ben Gurion Univ Negev, Dept Chem, IL-84105 Beer Sheva, Israel
基金:
欧洲研究理事会;
以色列科学基金会;
关键词:
ATOMIC LAYER DEPOSITION;
PHOTOELECTROCHEMICAL PERFORMANCE;
THIN-FILMS;
HEMATITE;
OXIDE;
CATALYST;
GROWTH;
PHOTOOXIDATION;
DYNAMICS;
D O I:
10.1021/ic403027r
中图分类号:
O61 [无机化学];
学科分类号:
070301 ;
081704 ;
摘要:
Hematite (alpha-Fe2O3) is one of most investigated oxides for energy applications and specifically for photocatalysis. Many approaches are used to prepare well-controlled films of hematite with good photocatalytic performance. However, most of these methods suffer from a number of disadvantages, such as the small quantities of the product, and the assembly of the nanostructures is usually a secondary process. Herein, we present a facile and large-scale synthesis of mesoporous hematite structures directly on various substrates at moderate temperature and study their photo-electrochemical (PEC) properties. Our approach is based on thermal decomposition of iron acetate directly on a substrate followed by an annealing process in air to produce a continuous mesoporous film of alpha-Fe2O3, with good control of the size of the pores. Improving the PEC properties of iron oxide was achieved by deposition of CoO domains, which were formed by thermal decomposition of cobalt acetate directly onto the hematite surface to produce alpha-Fe2O3/CoO nanostructures. PEC measurements of the hematite film before and after CoO growth were tested. Two methods were used to deposit the cobalt material: (a) thermal decomposition and (b) the most typically used method, adsorption of cobalt salt. The photocurrent of pure hematite was 0.25 mA/cm(2) at 1.23 V versus reversible hydrogen electrode (RHE), while modification of the hematite surface using the thermal decomposition method showed 180% improvement (0.7 mA/cm(2) at 1.23 V vs RHE) and 40% improvement (0.35 mA/cm(2) at 1.23 V vs RI-LE) via the adsorption method. Moreover, the onset potential was shifted by 130 and 70 mV when the surface of the hematite was modified by the thermal decomposition and adsorption methods, respectively.