Microstructure and phase stability of single crystal NiAl alloyed with Hf and Zr

被引:36
作者
Locci, IE
Dickerson, RM
Garg, A
Noebe, RD
Whittenberger, JD
Nathal, MV
Darolia, R
机构
[1] NASA, LEWIS RES CTR, CLEVELAND, OH 44135 USA
[2] NYMA INC, CLEVELAND, OH 44124 USA
[3] GE CO, AIRCRAFT ENGINES, CINCINNATI, OH 45215 USA
关键词
D O I
10.1557/JMR.1996.0384
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Six near stoichiometric, NiAl single-crystal alloys, with 0.05-1.5 at.% of Hf and Zr additions plus Si impurities, were microstructurally analyzed in the as-cast, homogenized, and aged conditions. Hafnium-rich interdendritic regions, containing the Heusler phase (Ni2AlHf), were found in all the as-cast alloys containing Hf. Homogenization heat treatments partially reduced these interdendritic segregated regions. Transmission electron microscopy (TEM) observations of the as-cast and homogenized microstructures revealed the presence of a high density of fine Hf (or Zr) and Si-rich precipitates. These were identified as G-phase, Ni(16)X(6)Si(7), or as an orthorhombic NiXSi phase, where X is Hf or Zr. Under these conditions the expected Heusler phase (beta') was almost completely absent. The Si responsible for the formation of the G and NiHfSi phases is the result of molten metal reacting with the Si-containing crucible used during the casting process. Varying the cooling rates after homogenization resulted in the refinement or complete suppression of the G and NiHfSi phases. In some of the alloys studied, long-term aging heat treatments resulted in the formation of Heusler precipitates, which were more stable at the aging temperature and coarsened at the expense of the G-phase. In other alloys, long-term aging resulted in the formation of the NiXSi phase. The stability of the Heusler or NiXSi phases can be traced to the reactive element (Hf or Zr) to silicon ratio, If the ratio is high, then the Heusler phase appears stable after long time aging. If the ratio is low, then the NiHfSi phase appears to be the stable phase.
引用
收藏
页码:3024 / 3038
页数:15
相关论文
共 30 条
[1]   EFFECT OF 0.1 AT-PERCENT ZIRCONIUM ON THE CYCLIC OXIDATION RESISTANCE OF BETA-NIAL [J].
BARRETT, CA .
OXIDATION OF METALS, 1988, 30 (5-6) :361-390
[2]  
DAROLIA R, 1993, STRUCTURAL INTERMETALLICS, P495
[3]   NIAL ALLOYS FOR HIGH-TEMPERATURE STRUCTURAL APPLICATIONS [J].
DAROLIA, R .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1991, 43 (03) :44-49
[4]  
DAROLIA R, 1992, NATO ADV SCI I E-APP, V213, P679
[5]   TRANSIENT OXIDATION OF SINGLE-CRYSTAL BETA-NIAL [J].
DOYCHAK, J ;
SMIALEK, JL ;
MITCHELL, TE .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1989, 20 (03) :499-518
[6]   Crystallography of the NiHfSi phase in a NiAl (0.5Hf) single-crystal alloy [J].
Garg, A ;
Noebe, RD ;
Darolia, R .
ACTA MATERIALIA, 1996, 44 (07) :2809-2820
[7]  
GARG A, 1995, 10178 NASA
[8]  
Gladyshevsky E., 1961, KRISTALLOGRAFIYA, V6, P769
[9]  
Gladyshevsky E I, 1963, RUSS J INORG CHEM, V8, P997
[10]  
Gladyshevsky E I, 1962, DOPOV AKAD NAUK UKR, V4, P481