Control and Characterization of the Structural, Electrical, and Optical Properties of Amorphous Zinc-Indium-Tin Oxide Thin Films

被引:81
作者
Buchholz, D. Bruce [1 ,2 ]
Liu, Jun [3 ]
Marks, Tobin J. [1 ,2 ,3 ]
Zhang, Ming [1 ,2 ]
Chang, Robert P. H. [1 ,2 ]
机构
[1] Northwestern Univ, Dept Mat Sci & Engn, Evanston, IL 60208 USA
[2] Northwestern Univ, Mat Res Ctr, Evanston, IL 60208 USA
[3] Northwestern Univ, Dept Chem, Evanston, IL 60208 USA
基金
美国国家科学基金会;
关键词
transparent conducting oxide; semiconductor; oxide; amorphous; TRANSPARENT CONDUCTING OXIDES; TRANSPORT-PROPERTIES; ELECTRONIC-STRUCTURE; HIGHLY TRANSPARENT; CARRIER TRANSPORT; O FILMS; SN-O; ZN; IN2O3; SEMICONDUCTORS;
D O I
10.1021/am900321f
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Zinc-indium-tin oxide (ZITO) films are grown by pulsed-laser deposition in which 30% of the indium in the In2O3 structure is replaced by substitution with zinc and tin in equal molar proportions In2-2xZnxSnxO3, where x = 0 3 Films grown at 25 and 100 degrees C exhibit electron diffraction patterns (EDPs) typical of amorphous materials At a deposition temperature of 200 degrees C. evidence of crystallinity begins to appear in the EDP data and becornes more evident in films deposited at 400 degrees C The advent of crystallinity affecis the electrical properties of the ZITO him, and the effect is ascribed to the boundaries between phases in the films The electrical and optical properties of the amorphous ZITO films grown at 25 degrees C are dependent on the oxygen partial pressure (P-o2) during film growth, transitioning from a high-mobility (36 cm(2)/V.s) conductor (sigma similar to 1700 S/cm) at P-o2 = 5 mTorr to a high-mobility semiconductor at Po-2 approximate to 20 mTorr Field-effect transistors (FETs) prepared with as-deposited amorphous ZITO channel layers on p(+)-Si/300 nm SiO2 substrates yield FETs with on/off ratios of 10(6), off currents of 10(-8) A, and field-effect saturation mobilities of 10 cm(2)/V s.
引用
收藏
页码:2147 / 2153
页数:7
相关论文
共 52 条
[1]   Variable-temperature electrical measurements of zinc oxide/tin oxide-cosubstituted indium oxide [J].
Ambrosini, A ;
Palmer, GB ;
Maignan, A ;
Poeppelmeier, KR ;
Lane, MA ;
Brazis, P ;
Kannewurf, CR ;
Hogan, T ;
Mason, TO .
CHEMISTRY OF MATERIALS, 2002, 14 (01) :52-57
[2]   Transparent conducting indium zinc tin oxide anode for highly efficient phosphorescent organic light emitting diodes [J].
Bae, Jung-Hyeok ;
Moon, Jong-Min ;
Jeong, Soon Wook ;
Kim, Jang-Joo ;
Kang, Jae-Wook ;
Kim, Do-Geun ;
Kim, Jong-Kuk ;
Park, Jeong-Woo ;
Kim, Han-Ki .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (01) :J1-J6
[3]   Influence of the semiconductor thickness on the electrical properties of transparent TFTs based on indium zinc oxide [J].
Barquinha, P. ;
Pimentel, A. ;
Marques, A. ;
Pereira, L. ;
Martins, R. ;
Fortunato, E. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2006, 352 (9-20) :1749-1752
[4]   ANOMALOUS OPTICAL ABSORPTION LIMIT IN INSB [J].
BURSTEIN, E .
PHYSICAL REVIEW, 1954, 93 (03) :632-633
[5]   High-performance ZnO thin-film transistors on gate dielectrics grown by atomic layer deposition [J].
Carcia, PF ;
McLean, RS ;
Reilly, MH .
APPLIED PHYSICS LETTERS, 2006, 88 (12)
[6]   High mobility transparent thin-film transistors with amorphous zinc tin oxide channel layer [J].
Chiang, HQ ;
Wager, JF ;
Hoffman, RL ;
Jeong, J ;
Keszler, DA .
APPLIED PHYSICS LETTERS, 2005, 86 (01) :013503-1
[7]   TRANSPARENT CONDUCTORS - A STATUS REVIEW [J].
CHOPRA, KL ;
MAJOR, S ;
PANDYA, DK .
THIN SOLID FILMS, 1983, 102 (01) :1-46
[8]  
Cui J, 2001, ADV MATER, V13, P1476, DOI 10.1002/1521-4095(200110)13:19<1476::AID-ADMA1476>3.0.CO
[9]  
2-Y
[10]   Transparent thin-film transistors with zinc indium oxide channel layer [J].
Dehuff, NL ;
Kettenring, ES ;
Hong, D ;
Chiang, HQ ;
Wager, JF ;
Hoffman, RL ;
Park, CH ;
Keszler, DA .
JOURNAL OF APPLIED PHYSICS, 2005, 97 (06)