共 61 条
Additive-Assisted Control over Phase-Separated Nanostructures by Manipulating Alkylthienyl Position at Donor Backbone for Solution-Processed, Non-Fullerene, All-Small-Molecule Solar Cells
被引:74
作者:
Huang, Jianhua
[1
]
Wang, Xue
[1
,2
]
Zhang, Xin
[1
]
Niu, Zhixiao
[1
,2
]
Lu, Zhenhuan
[1
]
Jiang, Bo
[1
]
Sun, Yuxi
[2
]
Zhan, Chuanlang
[1
]
Yao, Jiannian
[1
]
机构:
[1] Chinese Acad Sci, Inst Chem, CAS Key Lab Photochem, Beijing Natl Lab Mol Sci, Beijing 100190, Peoples R China
[2] QuFu Normal Univ, Key Lab Life Organ Anal, QuFu 273165, Peoples R China
关键词:
solution-processed;
non-fullerene;
all-small-molecule solar cell;
phase-separated nanostructure;
alkylthienyl position;
donor backbone;
OPEN-CIRCUIT VOLTAGE;
BAND-GAP;
PHOTOVOLTAIC PROPERTIES;
DEVICE PERFORMANCES;
ACCEPTOR MATERIALS;
EFFICIENT;
DIKETOPYRROLOPYRROLE;
TRIPHENYLAMINE;
OLIGOTHIOPHENE;
POLYMERS;
D O I:
10.1021/am406050j
中图分类号:
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
A non-fullerene, all-small-molecule solar cell (NF-SMSC) device uses the blend of a small molecule donor and a small molecule acceptor as the active layer. Aggregation ability is a key factor for this type of solar cell. Herein, we used the alkylthienyl unit to tune the aggregation ability of the diketopyrrolopyrrole (DPP)-based small molecule donors. Replacing two alkoxyl units in BDT-O-DPP with two alkylthienyl units yields BDT-T-DPP, and further introducing another two alkylthienyl units into the backbone produces BDT-T-2T-DPP. With the introduction of alkylthienyl, the backbone becomes twisted. As a result, the pi pi-stacking strength, aggregation ability, and crystallite size all obey the sequence of BDT-O-DPP > BDT-T-DPP > BDT-T-2T-DPP. When selected a reported perylene diimide dimer of bis-PDI-T-EG as acceptor, the best NF-SMSC device exhibits a power conversion efficiency of 1.34, 2.01, and 1.62%, respectively, for the BDT-O-DPP, BDT-T-DPP, and BDT-T-2T-DPP based system. The BDT-T-DPP/bis-PDI-T-EG system yields the best efficiency of 2.01% among the three combinations. This is due to the moderate aggregation ability of BDT-T-DPP yields moderate phase size of 30-50 nm, whereas the strong aggregation ability of BDT-O-DPP gives a bigger size of 50-80 nm, and the weak aggregation ability of BDT-T-2T-DPP produces a smaller size of 10-30 nm. The BDT-T-DPP/bis-PDI-T-EG combination exhibits balanced hole/electron mobility of 0.022/0.016 cm(2)/(V s), whereas the BDT-O-DPP/bis-PDI-T-EG and the BDT-T-2T-DPP/bis-PDI-T-EG blend show a hole/electron mobility of 0.0011/0.0057 cm(2)/(V s) and 0.0016/0.11 cm(2)/(V s), respectively.
引用
收藏
页码:3853 / 3862
页数:10
相关论文