摘要
In this paper we report on the synthesis and characterization of Ti3GeC2, Ti3Si0.5Ge0.5C2, and Ti3Si0.75Ge0.25C2 solid solutions. Polycrystalline, fully dense, predominantly single phase samples of Ti3Si0.5Ge0.5C2, Ti3Si0.75Ge0.25C2, and Ti3GeC2 of varying grain sizes were fabricated by reactive hot isostatic pressing (HIP) or hot pressing of Ti, C, SiC, and Ge powders. Based on the lattice parameter measurements we conclude that the extent of solid solubility in Ti-3(SixGe1-x)C-2 ranges for x = 0 to, at least, x = 0.75. Since the hardness values of both solid solution compositions (2.5 +/- 0.2 GPa) were in between those of Ti3SiC2 (3.0 +/- 0.3 GPa) and Ti3GeC2 (2.2 +/- 0.5 GPa) we conclude that no solid solution strengthening occurs in this system. All samples explored in this work were quite damage tolerant and thermal shock resistant. A 300 N Vickers indentation in a 1.5 mm thick, four-point bend bar decreases its strengths by anywhere from 25 to 35%. Quenching in water from 1000degreesC reduces the four-point flexural strength by 10 to 20%; i.e., it is not catastrophic. Notably, the post-quench flexural strength of the coarse-grained Ti3Si0.5Ge0.5C2 samples was approximate to25% higher than the as-received bars. Increasing the Ge content resulted in a decrease in the compressive strengths. The ultimate compressive strengths of fine-grained Ti3Si0.5Ge0.5C2 samples, decreased monotonically from room temperature to approximate to950degreesC. And while failure was brittle at room temperature, above 1000degreesC the loss in strength was more severe, but the deformation was more plastic. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:287 / 295
页数:9
相关论文
共 29 条
[1]  
*ASTM, 2000, 112 ASTM E
[2]  
*ASTM, C116194 ASTM
[3]   Electrical conductivity, thermopower, and hall effect of Ti3AIC2, Ti4AIN3, and Ti3SiC2 [J].
Barsoum, MW ;
Yoo, HI ;
Polushina, IK ;
Rud, VY ;
Rud, YV ;
El-Raghy, T .
PHYSICAL REVIEW B, 2000, 62 (15) :10194-10198
[4]   Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.5 [J].
Barsoum, MW ;
Ali, M ;
El-Raghy, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (07) :1857-1865
[5]  
Barsoum MW, 1997, J MATER SYNTH PROCES, V5, P197
[6]   The MN+1AXN phases:: A new class of solids;: Thermodynamically stable nanolaminates [J].
Barsoum, MW .
PROGRESS IN SOLID STATE CHEMISTRY, 2000, 28 (1-4) :201-281
[7]   Fully reversible, dislocation-based compressive deformation of Ti3SiC2 to 1GPa [J].
Barsoum, MW ;
Zhen, T ;
Kalidindi, SR ;
Radovic, M ;
Murugaiah, A .
NATURE MATERIALS, 2003, 2 (02) :107-111
[8]   Layered machinable ceramics for high temperature applications [J].
Barsoum, MW ;
Brodkin, D ;
ElRaghy, T .
SCRIPTA MATERIALIA, 1997, 36 (05) :535-541
[9]   Room-temperature ductile carbides [J].
Barsoum, MW ;
El-Raghy, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (02) :363-369
[10]   Dislocations, kink bands, and room-temperature plasticity of Ti3SiC2 [J].
Barsoum, MW ;
Farber, L ;
El-Raghy, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (07) :1727-1738