Cleaning of copper foil coated with sodium hexanoate as corrosion inhibitor

被引:14
作者
Bellakhal, N
Draou, K
Addou, A
Brisset, JL [1 ]
机构
[1] Univ Rouen, Lab Electrochim Interfaciale & Chim Analyt, F-76821 Mt St Aignan, France
[2] Univ Mostaganem, Dept Chim, Mostaganem, Algeria
关键词
copper; corrosion inhibitor; gliding arc plasma; humid air plasma; non-thermal plasma; sodium hexanoate; surface cleaning;
D O I
10.1023/A:1003964304448
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Sodium hexanoate is proposed as corrosion inhibitor for copper when the metal is situated in an aggressive aqueous or gaseous environment. The efficiency of the inhibitor, measured by electrochemical techniques in the ASTM 1384 standard solution, depends on the hexanoate concentration. Copper foils immersed in a (0.1 M) sodium hexanoate conditioning bath, and later exposed to a strongly oxidizing gliding arc plasma in humid air, yield oxide layers, the thickness and the nature of which differ from the unconditioned samples since the voltammograms show no CuO at the surface. The organic salt thus limits the oxidation process induced by the gaseous species. The organic layer remains active for at least 30 min. For longer exposures, the salt begins to degrade to carbon dioxide, which makes the plasma treatment a useful tool to clean metallic surfaces.
引用
收藏
页码:595 / 600
页数:6
相关论文
共 17 条
[11]   MODEL OF THE GLIDING ARC [J].
FRIDMAN, AA ;
PETROUSOV, A ;
CHAPELLE, J ;
CORMIER, JM ;
CZERNICHOWSKI, A ;
LESUEUR, H ;
STEVEFELT, J .
JOURNAL DE PHYSIQUE III, 1994, 4 (08) :1449-1465
[12]  
KUMBHAR AG, 1994, INDIAN J CHEM A, V33, P47
[13]  
Lesueur H, 1988, French patent, Patent No. [2639172, FR 2 639 172-A1]
[14]  
MORAS F, 1996, P 5 INT S HIGH PRESS, P87
[15]  
POUBAIX M, 1966, ATLAS ELECTROCHEMICA
[16]  
SHABAN A, 1994, P EUROCORR BOURNEMOU, V1, P112
[17]   CORRELATION OF SURFACE WETTABILITY AND CORROSION RATE FOR BENZOTRIAZOLE-TREATED COPPER [J].
THOMAS, RR ;
BRUSIC, VA ;
RUSH, BM .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1992, 139 (03) :678-685