Solubilisation of nickel from powders at near-neutral pH and the role of oxide layers

被引:8
作者
Pulvirenti, April L. [1 ]
Bishop, Elizabeth J. [1 ]
Adel-Hadadi, Mohamad A. [1 ]
Barkatt, Aaron [1 ]
机构
[1] Catholic Univ Amer, Dept Chem, Washington, DC 20064 USA
关键词
Nickel; XRD; Atmospheric corrosion; Oxidation; Passive films; ANODIC-DISSOLUTION; ELECTRON-SPECTROSCOPY; PASSIVE FILMS; OXIDATION; SURFACE; BEHAVIOR; IRON; TEMPERATURES; ADSORPTION; CORROSION;
D O I
10.1016/j.corsci.2009.05.029
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Dissolution rates of nickel powder in pH 5 acetate buffers were observed to be an effective indicator of the thickness of the oxide layer on the surface of the nickel particle. Tests on powders pre-cleaned with acid or pre-oxidized in air demonstrated this dependence. The saturation level of nickel in the solution is not greatly affected by the initial state of the powder. Effects of additive solutes are most pronounced during short-term dissolution tests. Among such solutes, reduced sulphur and selenium species, phosphate, fluoride, oxalate, and permanganate cause the largest increases in dissolution rate, while hexacyanoferrate, arsenite, periodate, chromate, vanadate, molybdate, iodate, and tungstate suppress the dissolution. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2043 / 2054
页数:12
相关论文
共 45 条
[1]   The influence of halide anions on the anodic behavior of nickel in borate solutions [J].
Abd El Aal, EE ;
Abd El Haleem, SM .
CHEMICAL ENGINEERING & TECHNOLOGY, 2005, 28 (10) :1158-1165
[2]  
Abd El Rehim S. S., 1986, Werkstoffe und Korrosion, V37, P550
[3]  
AESAR A, 2008, CATALOGUE MATERIALS
[4]   THE PASSIVATION OF NEWLY GENERATED SURFACE AND KINETICS OF ANODIC-DISSOLUTION OF NICKEL [J].
AGLADZE, T ;
KOLOTYRKIN, Y ;
JANIBAKHCHIEVA, L .
CORROSION SCIENCE, 1990, 31 :607-614
[5]   Steady-state anodic dissolution of iron in neutral and close-to-neutral media [J].
Aleksanyan, A. Yu. ;
Podobaev, A. N. ;
Reformatskaya, I. I. .
PROTECTION OF METALS, 2007, 43 (01) :66-69
[6]  
ALEKSANYAN AY, 2007, PROT MET+, V43, P135
[7]   The role of acrolein in the inhibition of the acid corrosion of iron with propargyl alcohol [J].
Avdeev, YG ;
Podobaev, NI .
PROTECTION OF METALS, 2005, 41 (06) :592-596
[8]   GROWTH OF A NICKEL-OXIDE LAYER ON A ROTATING NICKEL ELECTRODE IN A NON-BUFFERED SOLUTION OF SODIUM-SULFATE [J].
BARRAL, G ;
NJANJOEYOKE, F ;
MAXIMOVITCH, S .
ELECTROCHIMICA ACTA, 1995, 40 (06) :709-718
[9]   Study of electrochemically formed Ni(OH)(2) layers by EIS [J].
Barral, G ;
Maximovitch, S ;
NjanjoEyoke, F .
ELECTROCHIMICA ACTA, 1996, 41 (7-8) :1305-1311
[10]   CHARACTERIZATION OF THE PASSIVE LAYER AND OF HYDROXIDE DEPOSITS OF NICKEL BY IMPEDANCE SPECTROSCOPY [J].
BARRAL, G ;
NJANJOEYOKE, F ;
MAXIMOVITCH, S .
ELECTROCHIMICA ACTA, 1995, 40 (17) :2815-2828