Thermal-ageing of paraloid acrylic protective polymers

被引:108
作者
Lazzari, M [1 ]
Chiantore, O [1 ]
机构
[1] Univ Turin, IPM, Dept Chem, I-10125 Turin, Italy
关键词
thermal-ageing; thermal oxidation; acrylic resins;
D O I
10.1016/S0032-3861(99)00877-0
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal-ageing of a series of commercial acrylic/methacrylic resins, homo- and copolymers which are extensively used as stone protectives, has been investigated under conditions of constant temperatures at 110, 135 and 150 degrees C. Structural and molecular changes induced by the isothermal treatments in a forced-air circulation oven were followed by infrared and UV-Vis spectroscopy, and size exclusion chromatography (SEC), respectively. The stability of the resins appeared to be controlled by the reactivity of alkyl side groups, whose oxidative decomposition is favoured in the case of long ester groups, like the isobutyl and butyl ones. At the same time, the polymers containing long ester groups undergo fast and extensive cross-linking, together with loss of short chain fragments. In the acrylic/methacrylic resins where all or the majority of the alkyl side groups are short, chain scissions prevail over cross-linking and no insoluble fractions were formed. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:6447 / 6455
页数:9
相关论文
共 24 条
[21]  
ROHM H, TECHNICAL B
[22]  
Sims D., 1983, WEATHERING POLYM, DOI DOI 10.1002/POL.1984.130220709
[23]  
THOMSON G, 1975, CONSERVATION CULTURA, P303
[24]  
WYPICH G, 1995, HDB MAT WEATHERING