XRD measurement of mean thickness, thickness distribution and strain for illite and illite-smectite crystallites by the Bertaut-Warren-Averbach technique

被引:104
作者
Drits, VA
Eberl, DD
Srodon, J
机构
[1] RAN, Inst Geol, Moscow 109017, Russia
[2] US Geol Survey, Boulder, CO 80303 USA
[3] PAN, Inst Geol Sci, PL-31002 Krakow, Poland
关键词
crystallite; fundamental illite particles; illite; illite-smectite; MacEwan crystallites; mixed-layer clay; thickness distributions; Warren-Averbach method;
D O I
10.1346/CCMN.1998.0460105
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A modified version of the Bertaut-Warren-Averbach (BWA) technique (Bertaut 1949, 1950; Warren and Averbach 1950) has been developed to measure coherent scattering domain (CSD) sizes and strains in minerals by analysis of X-ray diffraction (XRD) data. This method is used to measure CSD thickness distributions for calculated and experimental XRD patterns of illites and illite-smectites (IS). The method almost exactly recovers CSD thickness distributions for calculated illite XRD patterns. Natural I-S samples contain swelling layers that lead to nonperiodic structures in the c* direction and to XRD peaks that are broadened and made asymmetric by mixed layering. Therefore, these peaks cannot be analyzed by the BWA method. These difficulties are overcome by K-saturation and heating prior to X-ray analysis in order to form 10-Angstrom periodic structures. BWA analysis yields the thickness distribution of mixed-layer crystals (coherently diffracting stacks of fundamental illite particles). For most IS samples, CSD thickness distributions can be approximated by lognormal functions. Mixed-layer crystal mean thickness and expandability then can be used to calculate fundamental illite particle mean thickness. Analyses of the dehydrated, K-saturated samples indicate that basal XRD reflections are broadened by symmetrical strain that may be related to local variations in smectite interlayers caused by dehydration, and that the standard deviation of the strain increases regularly with expandability. The 001 and 002 reflections are affected only slightly by this strain and therefore are suited for CSD thickness analysis. Mean mixed-layer crystal thicknesses for dehydrated I-S measured by the BWA method are very close to those measured by an integral peak width method.
引用
收藏
页码:38 / 50
页数:13
相关论文
共 32 条
[21]  
REYNOLDS RC, 1989, MODERN POWDER DIFFRA, P145
[22]  
Reynolds RobertC., 1985, NEWMOD COMPUTER PROG
[23]  
*SIEM, 1990, DIFFR 5000 POWD DIFF
[24]   CHEMISTRY OF ILLITE SMECTITE AND END-MEMBER ILLITE [J].
SRODON, J ;
MORGAN, DJ ;
ESLINGER, EV ;
EBERL, DD ;
KARLINGER, MR .
CLAYS AND CLAY MINERALS, 1986, 34 (04) :368-378
[25]   X-RAY-POWDER DIFFRACTION IDENTIFICATION OF ILLITIC MATERIALS [J].
SRODON, J .
CLAYS AND CLAY MINERALS, 1984, 32 (05) :337-349
[26]  
SRODON J, 1994, EUR J MINERAL, V6, P113
[27]   CHEMISTRY OF ILLITE-SMECTITE INFERRED FROM TEM MEASUREMENTS OF FUNDAMENTAL PARTICLES [J].
SRODON, J ;
ELSASS, F ;
MCHARDY, WJ ;
MORGAN, DJ .
CLAY MINERALS, 1992, 27 (02) :137-158
[29]   A NUMERICAL FOURIER-ANALYSIS METHOD FOR THE CORRECTION OF WIDTHS AND SHAPES OF LINES ON X-RAY POWDER PHOTOGRAPHS [J].
STOKES, AR .
PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON, 1948, 61 (346) :382-391
[30]   Hungarian investigations on the ''Zempleni'' illite [J].
Viczian, I .