Strength and toughness of tape-cast yttria-stabilized zirconia

被引:101
作者
Selçuk, A [1 ]
Atkinson, A [1 ]
机构
[1] Univ London Imperial Coll Sci Technol & Med, Dept Mat, London SW7 2BP, England
关键词
D O I
10.1111/j.1151-2916.2000.tb01507.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The biaxial flexural strength and fracture toughness of tape-cast yttria-stabilized zirconia, for application as the electrolyte in solid oxide fuel cells, have been measured at room temperature and at a typical operating temperature of 900 degrees C. The flexural strength was measured in ring-on-ring loading and decreased from 416 MPa at room temperature to 265 MPa at 900 degrees C. The fracture toughness was measured using two different techniques: Indentation fracture and double-torsion loading. The latter was more reliable and gave a fracture toughness of 1.61 +/- 0.12 MPa.m(1/2) at room temperature and 1.02 +/- 0.05 MPa.m(1/2) at 900 degrees C. The flexural strength and fracture toughness were quantitatively consistent with fracture being initiated at the observed surface defects. The lower fracture toughness at 900 degrees C is partly due to a reduction in elastic modulus and partly due to a reduction in the work of fracture.
引用
收藏
页码:2029 / 2035
页数:7
相关论文
共 25 条
[11]   NEW FORMULA FOR INDENTATION TOUGHNESS IN CERAMICS [J].
LAUGIER, MT .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1987, 6 (03) :355-356
[12]  
LOWRIE FL, 1996, THESIS U LONDON LOND
[13]   CERAMIC FUEL-CELLS [J].
MINH, NQ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (03) :563-588
[14]  
Munro RG, 1997, J AM CERAM SOC, V80, P1919, DOI 10.1111/j.1151-2916.1997.tb03074.x
[15]  
MURRAY MJ, 1977, J AUST I MET, V22, P126
[16]  
NEWMAN JC, 1981, ENG FRACT MECH, V15
[17]   EVALUATION OF KLC OF BRITTLE SOLIDS BY THE INDENTATION METHOD WITH LOW CRACK-TO-INDENT RATIOS [J].
NIIHARA, K ;
MORENA, R ;
HASSELMAN, DPH .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1982, 1 (01) :13-16
[18]  
OUTWATER JO, 1974, ASTM STP, V559, P127
[19]  
PONTON CB, 1989, MATER SCI TECH SER, V5, P865, DOI 10.1179/026708389790222852
[20]  
PONTON CB, 1989, MATER SCI TECH SER, V5, P961, DOI 10.1179/026708389790339574