Review of the high-temperature oxidation of iron and carbon steels in air or oxygen

被引:558
作者
Chen, RY
Yuen, WYD
机构
[1] BHP Steel, Western Port Works, Hastings, Vic 3915, Australia
[2] BHP Steel, Res Labs, Port Kembla, NSW 2505, Australia
来源
OXIDATION OF METALS | 2003年 / 59卷 / 5-6期
关键词
high-temperature oxidation; iron; steel; wustite; magnetite; hematite;
D O I
10.1023/A:1023685905159
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper reviews previous studies on iron and steel oxidation in oxygen or air at high temperatures. Oxidation of iron at temperatures above 700degreesC follows the parabolic law with the development of a three-layered hematite/magnetite/wustite scale structure. However, at temperatures below 700degreesC, inconsistent results have been reported, and the scale structures are less regular, significantly affected by sample-preparation methods. Oxidation of carbon steel is generally slower than iron oxidation. For very short-time oxidation, the scale structures are similar to those formed on iron, but for longer-time oxidation, because of the less adherent nature, the scale structures developed are typically much more complex. Continuous-cooling conditions, after very short-time oxidation, favor the retention of an adherent scale, suggesting that the method proposed by Kofstad for deriving the rate constant using continuous cooling or heating-oxidation data is more appropriate for steel oxidation. Oxygen availability has certain effects on iron and steel oxidation. Under continuous cooling conditions, the final scale structure is found to be a function of the starting temperature for cooling and the cooling rate. Different scale structures develop across the width of a hot-rolled strip because of the varied oxygen availability and cooling rates at different locations.
引用
收藏
页码:433 / 468
页数:36
相关论文
共 152 条
[21]  
BROWNE KM, 1993, STEEL TIMES DEC, P524
[22]   EFFECT OF COLD WORK ON OXIDATION OF IRON FROM 400-650 DEGREES C [J].
CAPLAN, D ;
COHEN, M .
CORROSION SCIENCE, 1966, 6 (07) :321-&
[23]   OXIDATION OF FE-C ALLOYS AT 500-DEGREES-C [J].
CAPLAN, D ;
SPROULE, GI ;
HUSSEY, RJ ;
GRAHAM, MJ .
OXIDATION OF METALS, 1978, 12 (01) :67-82
[24]   OVERTEMPERATURE IN METAL SCALING [J].
CAPLAN, D .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1960, 107 (04) :359-360
[25]   COMPARISON OF KINETICS OF HIGH-TEMPERATURE OXIDATION OF FE AS INFLUENCED BY METAL PURITY AND COLD WORK [J].
CAPLAN, D ;
SPROULE, GI ;
HUSSEY, RJ .
CORROSION SCIENCE, 1970, 10 (01) :9-&
[26]   OXIDATION OF FE-C ALLOYS AT 700-DEGREES-C [J].
CAPLAN, D ;
SPROULE, GI ;
HUSSEY, RJ ;
GRAHAM, MJ .
OXIDATION OF METALS, 1979, 13 (03) :255-272
[27]  
Caplan D., 1963, CORROS SCI, V3, P139, DOI DOI 10.1016/S0010-938X(63)80084-0
[28]   EFFECT OF METALLURGICAL PRETREATMENT ON KINETICS OF OXIDATION OF IRON AT 700DEGREES C IN PURE GASEOUS OXYGEN [J].
CARPENTER, DL ;
RAY, AC .
CORROSION SCIENCE, 1973, 13 (06) :493-+
[29]  
Chaudron G, 1924, CR HEBD ACAD SCI, V178, P2173
[30]  
CHAUDRON G, 1951, REV METALL, V48, P917