The air oxidation of two-phase Cu-Cr alloys at 700-900°C

被引:70
作者
Niu, Y
Gesmundo, F
Viani, F
Douglass, DL
机构
[1] Univ Genoa, Fac Ingn, Ist Chim, I-16129 Genoa, Italy
[2] Inst Corros & Protect Met CAS, State Key Lab Corros, Shenyang 110015, Peoples R China
[3] Univ Arizona, Arizona Mat Lab, Tucson, AZ 85712 USA
来源
OXIDATION OF METALS | 1997年 / 48卷 / 5-6期
关键词
chromium; copper; binary alloys; two-phase alloys; oxidation; high temperatures;
D O I
10.1007/BF02153456
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The oxidation in air of three two-phase Cu-Cr alloys with nominal Cr contents of 25, 50, and 75 wt. % was studied at 700-900 degrees C. The alloys corroded nearly parabolically, except at 900 degrees C, when the corrosion rates decreased with time more rapidly than predicted by the parabolic rate law. The corrosion rate decreased for higher Cr contents in the alloy under constant temperature and generally increased with temperature for the same alloy composition. The scales were complex and consisted in most cases of an outermost copper oxide layer free fr om chromium and an inner layer composed of a matrix of copper oxide or of the double oxide Cu2Cr2O4, often containing particles of chromium metal surrounded by chromia and then by the double oxide, Metallic copper was also frequently mixed with chromia. Cr-rich regions tended to form continuous chromia layers at the base of the scale, especially at the highest temperature. No chromium depletion was observed in the alloy.
引用
收藏
页码:357 / 380
页数:24
相关论文
共 46 条
[11]  
GESMUNDO F, 1994, OXID MET, V42, P409
[12]   THE TRANSITION FROM THE FORMATION OF MIXED SCALES TO THE SELECTIVE OXIDATION OF THE MOST-REACTIVE COMPONENT IN THE CORROSION OF SINGLE AND 2-PHASE BINARY-ALLOYS [J].
GESMUNDO, F ;
VIANI, F ;
NIU, Y ;
DOUGLASS, DL .
OXIDATION OF METALS, 1993, 40 (3-4) :373-393
[13]   The internal oxidation of two-phase binary alloys under low oxidant pressures [J].
Gesmundo, F ;
Viani, F ;
Niu, Y .
OXIDATION OF METALS, 1996, 45 (1-2) :51-76
[14]   FURTHER ASPECTS OF THE OXIDATION OF BINARY 2-PHASE ALLOYS [J].
GESMUNDO, F ;
VIANI, F ;
NIU, Y ;
DOUGLASS, DL .
OXIDATION OF METALS, 1993, 39 (3-4) :197-209
[15]   OXIDATION BEHAVIOR OF 2-PHASE ALLOY FE-44 W-O CU [J].
GESMUNDO, F ;
NANNI, P ;
WHITTLE, DP .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (08) :1773-1782
[16]   OXIDATION OF MULTICOMPONENT 2-PHASE ALLOYS [J].
GESMUNDO, F ;
GLEESON, B .
OXIDATION OF METALS, 1995, 44 (1-2) :211-237
[17]  
GESMUNDO F, 1985, REACTIVITY SOLIDS A, V28, P175
[18]   MICROSTRUCTURE, ADHESION AND GROWTH-KINETICS OF PROTECTIVE SCALES ON METALS AND ALLOYS [J].
HINDAM, H ;
WHITTLE, DP .
OXIDATION OF METALS, 1982, 18 (5-6) :245-284
[19]   THE OXIDATION OF NI-70 WT-PERCENT-CR IN OXYGEN BETWEEN 1073-DEGREES-K AND 1473-DEGREES-K [J].
HODGKIESS, T ;
WOOD, GC ;
WHITTLE, DP ;
BASTOW, BD .
OXIDATION OF METALS, 1980, 14 (03) :263-277
[20]  
Kofstad P., 1988, Elsevier Appl. Sci., V24, DOI [10.1002/crat.2170240408, DOI 10.1002/CRAT.2170240408]