Electrochemical reactivity of Mg2Sn phases with metallic lithium

被引:30
作者
Larcher, D [1 ]
Prakash, AS [1 ]
Saint, J [1 ]
Morcrette, M [1 ]
Tarascon, JM [1 ]
机构
[1] Univ Picardie, CNRS UMR 6007, Lab Reactivite & Chim Solides, F-80039 Amiens, France
关键词
D O I
10.1021/cm040132h
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Stable (c) and metastable (h) forms Of Mg2Sn were prepared as crystallized phases by ball-milling of elemental powders. Through in situ X-ray diffraction measurements, we deduced the reactivity mechanisms Of c-Mg2Sn toward lithium. It entails first a monophasic insertion of about one lithium per formula unit into the fcc Sn framework without extrusion of either Mg or Sn, then a biphasic process leading to the formation of cubic Li2MgSn concomitant with a progressive expulsion of Mg, and finally the formation of Li-Mg solid-solution alloys. Upon charging, the poor reversibility of the alloying reaction of Li with Mg leads to a deficit in free Mg, resulting in the formation of a Mg2Sn + Sn mixture, and accounting for the poor cyclability Of Mg2Sn/Li cells over the 0.0-1.5 V voltage window. Limiting the cycling to the monophasic process was shown to improve the cycling behavior. Finally, we found that the electrochemical reaction of h-Mg2Sn with Li leads to the same Li2MgSn intermediate and the same subsequent sequence of transformations, resulting in similarly poor capacity retention upon cycling.
引用
收藏
页码:5502 / 5511
页数:10
相关论文
共 38 条
[31]   Intermetallic insertion electrodes derived from NiAs-, Ni2In-, and Li2CuSn-type structures for lithium-ion batteries [J].
Thackeray, MM ;
Vaughey, JT ;
Kahaian, AJ ;
Kepler, KD ;
Benedek, R .
ELECTROCHEMISTRY COMMUNICATIONS, 1999, 1 (3-4) :111-115
[32]   Metastable hexagonal Mg2Sn obtained by mechanical alloying [J].
Urretavizcaya, G ;
Meyer, GO .
JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 339 (1-2) :211-215
[33]  
Vaughey JT, 2000, ELECTROCHEM SOLID ST, V3, P13, DOI 10.1149/1.1390944
[34]   Ionic diffusion in a ternary superionic conductor: An ab initio molecular dynamics study [J].
Wengert, S ;
Nesper, R ;
Andreoni, W ;
Parrinello, M .
PHYSICAL REVIEW LETTERS, 1996, 77 (25) :5083-5085
[35]   A room temperature study of the binary lithium-silicon and the ternary lithium-chromium-silicon system for use in rechargeable lithium batteries [J].
Weydanz, WJ ;
Wohlfahrt-Mehrens, M ;
Huggins, RA .
JOURNAL OF POWER SOURCES, 1999, 81 :237-242
[36]   LITHIUM INSERTION IN CARBONS CONTAINING NANODISPERSED SILICON [J].
WILSON, AM ;
DAHN, JR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (02) :326-332
[37]   Si/C composites for high capacity lithium storage materials [J].
Yang, J ;
Wang, BF ;
Wang, K ;
Liu, Y ;
Xie, JY ;
Wen, ZS .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2003, 6 (08) :A154-A156
[38]   Small particle size multiphase Li-alloy anodes for lithium-ion-batteries [J].
Yang, J ;
Winter, M ;
Besenhard, JO .
SOLID STATE IONICS, 1996, 90 (1-4) :281-287