The durability of E-glass vinyl ester composite materials subjected to environmental conditioning and sustained loading

被引:31
作者
Buck, SE [1 ]
Lischer, DW [1 ]
Nemat-Nasser, S [1 ]
机构
[1] Univ Calif San Diego, Dept Appl Mech & Engn Sci, Ctr Excellence Adv Mat, La Jolla, CA 92093 USA
关键词
D O I
10.1177/002199839803200904
中图分类号
TB33 [复合材料];
学科分类号
摘要
A series of experiments has been performed to observe the effects of the combination of sustained load, elevated temperature, and moisture on the durability of an E-glass/vinyl ester composite material. This durability is evaluated in terms of the ultimate tensile strength of the material. The results have confirmed that moisture at elevated temperatures reduces the ultimate tensile strength of the material, as reported in previous studies. In these experiments, a sustained load has been applied to samples during the conditioning process and has been found to further reduce the composite durability. Conditioning also decreases the strain to failure, with a greater decrease overall for samples which were loaded during conditioning.
引用
收藏
页码:874 / 892
页数:19
相关论文
共 35 条
[21]  
MANDELL JF, 1977, R774 MIT
[22]   DAMAGE CHARACTERISTICS IN NOTCHED CARBON-FIBER COMPOSITES SUBJECTED TO FATIGUE LOADING - ENVIRONMENTAL-EFFECTS [J].
MORTON, J ;
KELLAS, S ;
BISHOP, SM .
JOURNAL OF COMPOSITE MATERIALS, 1988, 22 (07) :657-673
[23]   Flexural strength and interlaminar shear strength of stitched GRP laminates following repeated impacts [J].
Mouritz, AP ;
Gallagher, J ;
Goodwin, AA .
COMPOSITES SCIENCE AND TECHNOLOGY, 1997, 57 (05) :509-522
[24]   Acid resistance of glass fibre composites with different layup sequencing .1. Diffusion studies [J].
Pai, R ;
Kamath, MS ;
Rao, RMVGK .
JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1997, 16 (11) :1002-1012
[25]   Acid resistance of glass fibre composites with different layup sequencing .2. Degradation studies [J].
Pai, R ;
Kamath, MS ;
Rao, RMVGK .
JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1997, 16 (11) :1013-1019
[26]  
REHFIELD LW, 1982, ASTM STP, V768, P148
[27]   INFLUENCE OF WATER-UPTAKE ON INTERLAMINAR FRACTURE PROPERTIES OF CARBON-FIBER-REINFORCED POLYMER COMPOSITES [J].
SELZER, R ;
FRIEDRICH, K .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (02) :334-338
[28]  
SERAFINI TT, 1982, ASTM STP, V768, P5
[29]   THE EFFECT OF SEAWATER EXPOSURE ON MODE-I INTERLAMINAR FRACTURE AND CRACK-GROWTH IN GRAPHITE EPOXY [J].
SLOAN, FE ;
SEYMOUR, RJ .
JOURNAL OF COMPOSITE MATERIALS, 1992, 26 (18) :2655-2673
[30]   ENVIRONMENTAL-EFFECTS ON GLASS-FIBER REINFORCED POLYESTER AND VINYLESTER COMPOSITES [J].
SPRINGER, GS ;
SANDERS, BA ;
TUNG, RW .
JOURNAL OF COMPOSITE MATERIALS, 1980, 14 (JUL) :213-232