Three-dimensional hydrogen microscopy in diamond

被引:100
作者
Reichart, P
Datzmann, G
Hauptner, A
Hertenberger, R
Wild, C
Dollinger, G
机构
[1] Tech Univ Munich, Phys Dept E12, D-85748 Garching, Germany
[2] Univ Munich, Dept Phys, D-85748 Garching, Germany
[3] Fraunhofer Inst Appl Solid State Phys, D-79108 Freiburg, Germany
关键词
D O I
10.1126/science.1102910
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
A microprobe of protons with an energy of 17 million electron volts is used to quantitatively image three-dimensional hydrogen distributions at a lateral resolution better than 1 micrometer with high sensitivity. Hydrogen images of a <110>-textured undoped potycrystalline diamond film show that most of the hydrogen is located at grain boundaries. The average amount of hydrogen atoms along the grain boundaries is (8.1 +/- 1.5) x 10(14) per square centimeter, corresponding to about a third of a monolayer. The hydrogen content within the grain is below the experimental sensitivity of 1.4 x 10(16) atoms per cubic centimeter (0.08 atomic parts per million). The data prove a low hydrogen content within chemical vapor deposition-grown diamond and the importance of hydrogen at grain boundaries, for example, with respect to electronic properties of polycrystalline diamond.
引用
收藏
页码:1537 / 1540
页数:4
相关论文
共 33 条
[1]   LOW-PRESSURE, METASTABLE GROWTH OF DIAMOND AND DIAMONDLIKE PHASES [J].
ANGUS, JC ;
HAYMAN, CC .
SCIENCE, 1988, 241 (4868) :913-921
[2]   Deuterium depth profiles at CVD diamond surfaces [J].
Bergmaier, A ;
Dollinger, G ;
Aleksov, A ;
Gluche, P ;
Kohn, E .
SURFACE SCIENCE, 2001, 481 (1-3) :L433-L436
[3]  
Bergonzo P, 2001, PHYS STATUS SOLIDI A, V185, P167, DOI 10.1002/1521-396X(200105)185:1<167::AID-PSSA167>3.0.CO
[4]  
2-F
[5]   NONDESTRUCTIVE ANALYSIS FOR TRACE AMOUNTS OF HYDROGEN [J].
COHEN, BL ;
DEGNAN, JH ;
FINK, CL .
JOURNAL OF APPLIED PHYSICS, 1972, 43 (01) :19-&
[6]   A study of the mobility and trapping of minor hydrogen concentrations in diamond in three dimensions using quantitative ERDA microscopy [J].
Connell, SH ;
Sellschop, JPF ;
Butler, JE ;
Maclear, RD ;
Doyle, BP ;
Machi, IZ .
DIAMOND AND RELATED MATERIALS, 1998, 7 (11-12) :1714-1718
[7]   The Munich microprobe SNAKE:: First results using 20 MeV protons and 90 MeV sulfur ions [J].
Datzmann, G ;
Dollinger, G ;
Goeden, C ;
Hauptner, A ;
Körner, HJ ;
Reichart, P ;
Schmelmer, O .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2001, 181 :20-26
[8]   HYDROGEN IN POLYCRYSTALLINE DIAMOND - AN INFRARED-ANALYSIS [J].
DISCHLER, B ;
WILD, C ;
MULLERSEBERT, W ;
KOIDL, P .
PHYSICA B-CONDENSED MATTER, 1993, 185 (1-4) :217-221
[9]  
DISCHLER B, 1998, SPRINGER SERIES MAT, V11
[10]   IMPURITIES OF LIGHT-ELEMENTS IN CVD DIAMOND [J].
DOLLINGER, G ;
BERGMAIER, A ;
FREY, CM ;
ROESLER, M ;
VERHOEVEN, H .
DIAMOND AND RELATED MATERIALS, 1995, 4 (5-6) :591-595