FTIR analysis of cellulose treated with sodium hydroxide and carbon dioxide

被引:834
作者
Oh, SY
Yoo, DI [1 ]
Shin, Y
Seo, G
机构
[1] Chonnam Natl Univ, Dept Text Engn, Kwangju 500757, South Korea
[2] Chonnam Natl Univ, Dept Clothing & Text, Kwangju 500757, South Korea
[3] Chonnam Natl Univ, Dept Chem Engn, Kwangju 500757, South Korea
关键词
cellulose; sodium cellulose; carbon dioxide; FTIR; hydrogen-bond intensity (HBI); crystallinity index (CI); carbonate ion;
D O I
10.1016/j.carres.2004.11.027
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Cellulose samples treated with sodium hydroxide (NaOH) and carbon dioxide in dimethylacetamide (DMAc) were analyzed by FTIR spectroscopy. Absorbance of hydrogen-bonded OH stretching was considerably decreased by the treatment of NaOH and carbon dioxide. The relative absorbance ratio (A(4000-2995)/A(993)) represented the decrease of absorbance as a criterion of hydrogen-bond intensity (HBI). The absorbance of the band at 1430 cm(-1) due to a crystalline absorption was also decreased by NaOH treatment. The absorbance ratio of the bands at 1430 and 987-893 cm(-1) (A(1430)/A(900)), adopted as crystallinity index (CI), was closely related to the portion of cellulose I structure. With the help of FTIR equipped with an on-line evacuation apparatus, broad OH bending due to bound water could be eliminated. FTIR spectra of the carbon dioxide-treated cellulose samples at 1700-1525 cm(-1) were divided into some bands including 1663, 1635, 1616, and 1593 cm(-1). The broad OH bending due to bound water at 1641-1645 cm(-1) was resolved to two bands at 1663 and 1635 cm(-1). As a trace of DMAc, the band at 1616 cm(-1) is disappeared by washing for the cellulose treated with carbon dioxide (Cell 1-C and Cell 2/60-C). The decrease of HBI, the easy removal of DMAc, and the band at 1593 cm(-1) supported the introduction of new chemical structure in cellulose. The bands shown at 1593 and 1470 cm(-1) was assigned as hydrogen-bonded, carbonyl stretching and O-C-O stretching of the carbonate ion. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:417 / 428
页数:12
相关论文
共 20 条
[11]  
OCONNOR RT, 1958, TEXT RES J, V28, P383
[12]   Preparation of regenerated cellulose fiber via carbonation. I. Carbonation and dissolution in an aqueous NaOH solution [J].
Oh, SY ;
Yoo, DI ;
Shin, Y ;
Lee, WS ;
Jo, SM .
FIBERS AND POLYMERS, 2002, 3 (01) :1-7
[13]   The association of water to cellulose and hemicellulose in paper examined by FTIR spectroscopy [J].
Olsson, AM ;
Salmén, L .
CARBOHYDRATE RESEARCH, 2004, 339 (04) :813-818
[14]   FT-IR and FT-Raman study of hydrothermally degradated cellulose [J].
Proniewicz, LM ;
Paluszkiewicz, C ;
Weselucha-Birczynska, A ;
Majcherczyk, H ;
Baranski, A ;
Konieczna, A .
JOURNAL OF MOLECULAR STRUCTURE, 2001, 596 :163-169
[15]   Characterisation of the substituent distribution in starch and cellulose derivatives [J].
Richardson, S ;
Gorton, L .
ANALYTICA CHIMICA ACTA, 2003, 497 (1-2) :27-65
[16]   IR spectroscopy in catalysis [J].
Ryczkowski, J .
CATALYSIS TODAY, 2001, 68 (04) :263-381
[17]   Effects of short-time vibratory ball milling on the shape of FT-IR spectra of wood and cellulose [J].
Schwanninger, M ;
Rodrigues, JC ;
Pereira, H ;
Hinterstoisser, B .
VIBRATIONAL SPECTROSCOPY, 2004, 36 (01) :23-40
[18]  
VASILE C, 2004, EUR POLYM J, P1
[19]  
WADSWORTH LC, 1987, CELLULOSE ITS DERIVA, P344
[20]  
YAMASHIKI T, 1990, E H S POLYM, P197