An overview of the machinability of aeroengine alloys

被引:827
作者
Ezugwu, EO
Bonney, J
Yamane, Y
机构
[1] S Bank Univ, Sch Engn, Machining Res Ctr, London SE1 0AA, England
[2] Hiroshima Univ, Dept Engn, Higashihiroshima 7398527, Japan
关键词
machinability; aeroengine alloys; titanium; nickel-based alloys;
D O I
10.1016/S0924-0136(02)01042-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Advanced materials such as aeroengine alloys, structural ceramics and hardened steel provide a serious challenge for cutting tool materials during machining due to their unique combinations of properties such as high temperature strength, hardness and chemical wear resistance. Although these properties are desirable design requirements, they pose a greater challenge to manufacturing engineers due to the high temperatures and stresses generated during machining. The poor thermal conductivity of these alloys result in concentration of high temperatures at the tool-workpiece interface. This is worsened at higher cutting conditions because of the significant reduction in the strength and hardness of the cutting tool. This weakens the bonding strength of the tool substrate, thereby accelerating tool wear by mechanical (abrasion and attrition) and thermally related (diffusion and plastic deformation) mechanisms. Therefore, cutting tools used for machining aerospace materials must be able to maintain their hardness and other mechanical properties at higher cutting temperatures encountered in high speed machining. Tool materials with improved hardness like cemented carbides (including coated carbides), ceramics and cubic boron nitride (CBN) are the most frequently used for machining aeroengine alloys. Despite the superior hardness and cutting performance of CBN tools, ceramic tools are generally preferred for high speed continuous machining because of their much lower cost. Improvements in machining productivity can also be achieved with the latest machining techniques such as ramping or taper turning and rotary machining. These techniques often minimise or completely eliminate the predominant notching of the cutting tools, consequently resulting in catastrophic fracture of the entire cutting edge when machining aeroengine alloys. (C) 2002 Elsevier Science B.V All rights reserved.
引用
收藏
页码:233 / 253
页数:21
相关论文
共 93 条
[81]   Ceramics superplasticity [J].
Wakai, F ;
Kondo, N ;
Shinoda, Y .
CURRENT OPINION IN SOLID STATE & MATERIALS SCIENCE, 1999, 4 (05) :461-465
[82]   Evaluation of a self-propelled rotary tool in the machining of aerospace materials [J].
Wang, ZM ;
Ezugwu, EO ;
Gupta, A .
TRIBOLOGY TRANSACTIONS, 1998, 41 (02) :289-295
[83]  
WANG ZM, 1997, THESIS S BANK U
[84]   Cryogenic machining of hard-to-cut materials [J].
Wang, ZY ;
Rajurkar, KP .
WEAR, 2000, 239 (02) :168-175
[85]   Wear of CBN tool in turning of silicon nitride with cryogenic cooling [J].
Wang, ZY ;
Rajurkar, KP .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 1997, 37 (03) :319-326
[86]  
Wertheim R., 1992, CIRP Ann.-Manuf. Technol, V41, P101, DOI DOI 10.1016/S0007-8506(07)61162-7
[87]   Superplasticity in a fine-grained beta-silicon nitride ceramic containing a transient liquid [J].
Xie, RJ ;
Mitomo, M ;
Zhan, GD .
ACTA MATERIALIA, 2000, 48 (09) :2049-2058
[88]   Research and development of rare-earth cemented carbides [J].
Xu, CH ;
Ai, X ;
Huang, CZ .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2001, 19 (03) :159-168
[89]  
XUEBING H, 1998, MATER LETT, V36, P210
[90]   The deformation mechanisms of superplastic flow in fine-grained beta-silicon nitride ceramics [J].
Zhan, GD ;
Mitomo, M ;
Xie, RJ ;
Kurashima, K .
ACTA MATERIALIA, 2000, 48 (09) :2373-2382