Capacity fading of LiMn2O4 electrode synthesized by the emulsion drying method

被引:66
作者
Myung, ST
Chung, HT
Komaba, S
Kumagai, N
Gu, HB
机构
[1] Iwate Univ, Fac Engn, Dept Appl Chem & Mol Sci, Morioka, Iwate 0208551, Japan
[2] Dongshin Univ, Fac Engn, Dept Ceram Engn, Naju 520714, Chonnam, South Korea
[3] Chonnam Natl Univ, Fac Engn, Dept Elect Engn, Puk Gu, Kwangju 500757, South Korea
关键词
emulsion drying method; LiMn2O4; capacity fading; particle disruption;
D O I
10.1016/S0378-7753(00)00455-9
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
We adapted the emulsion drying method to obtain highly crystalline spinel LiMn2O4 phase using LiNO3 and Mn(NO3)(2) . 6H(2)O as starting materials. The emulsion-dried powders were calcined at various temperatures for 24 h in air, and their crystalline phases were identified as a cubic spinel structure with the space group Fd3m by X-ray diffraction study. The initial discharge capacity of the samples calcined at 650 degrees C, 750 degrees C and 850 degrees C were approximately 120 mA h/g, irrespective of calcination temperature. However, their capacity fadings were significantly dependent on the calcination temperature. To investigate the structural changes in the oxide cathode, XRD experiment was carried out as functions of lithium content and charge-discharge cycling number. Through the SEM observation, it was found that particles were disrupted, and the degree of disruption increased with lithium content and cycling. (C) 2000 Elsevier Science S.A. All rights reserved.