Delocalized free electron densities in degraded polystyrene and polypropylene macroradicals: The source of different photooxidation rates

被引:21
作者
Shyichuk, A
Melnyk, D
White, JR
机构
[1] Univ Technol & Agr, Fac Chem Technol & Engn, PL-85326 Bydgoszcz, Poland
[2] PreCarpathian Univ, Bioorgan Chem Dept, UA-76000 Ivano Frankivsk, Ukraine
[3] Newcastle Univ, Sch Chem Engn & Adv Mat, Div Mat, Newcastle Upon Tyne NE1 7RU, Tyne & Wear, England
关键词
macroradical; free spin; delocalization; photooxidation; polystyrene; polypropylene;
D O I
10.1002/pola.10645
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Electron structures of alkyl, alkoxy, and peroxy macroradicals for both polypropylene and polystyrene have been studied with quantum chemical methods. The polystyrene tertiary alkoxy macroradical has full delocalization of free spin on a neighboring aromatic ring. In addition, the spin is quite delocalized. on polystyrene tertiary alkoxy macroradicals and also on both secondary and tertiary peroxy macroradicals. Such strong delocalization does not occur with polypropylene macroradicals, and it is proposed that the inactivation of polystyrene macroradicals caused by spin delocalization is the reason that polystyrene photodegradation rates are slower than those of polypropylene. (C) 2003 Wiley Periodicals, Inc.
引用
收藏
页码:1070 / 1076
页数:7
相关论文
共 16 条
[1]   Simultaneous FTIR emission spectroscopy and chemiluminescence of oxidizing polypropylene: Evidence for alternate chemiluminescence mechanisms [J].
Blakey, I ;
George, GA .
MACROMOLECULES, 2001, 34 (06) :1873-1880
[2]   Mechanism and molecular weight model for thermal oxidation of linear ethylene-butene copolymer [J].
Chiantore, O ;
Tripodi, S ;
Sarmoria, C ;
Vallés, E .
POLYMER, 2001, 42 (09) :3981-3987
[3]   Photooxidation of fire retarded polypropylene [J].
Gardette, JL ;
Sinturel, C ;
Lemaire, J .
POLYMER DEGRADATION AND STABILITY, 1999, 64 (03) :411-417
[4]   PHOTOOXIDATION MECHANISMS OF STYRENIC POLYMERS [J].
GARDETTE, JL ;
MAILHOT, B ;
LEMAIRE, J .
POLYMER DEGRADATION AND STABILITY, 1995, 48 (03) :457-470
[5]   Thermo-oxidative degradation of isotactic polypropylene at high temperatures: phenolic antioxidants versus HAS [J].
Gensler, R ;
Plummer, CJG ;
Kausch, HH ;
Kramer, E ;
Pauquet, JR ;
Zweifel, H .
POLYMER DEGRADATION AND STABILITY, 2000, 67 (02) :195-208
[6]   Molecular weight changes during the photooxidation of isotactic polypropylene [J].
Girois, S ;
Audouin, L ;
Verdu, J ;
Delprat, P ;
Marot, G .
POLYMER DEGRADATION AND STABILITY, 1996, 51 (02) :125-132
[7]   Submicrometric characterization of the heterogeneous photooxidation of polypropylene by microthermal analysis [J].
Grossetete, T ;
Gonon, L ;
Verney, V .
POLYMER DEGRADATION AND STABILITY, 2002, 78 (02) :203-210
[8]   Using molecular weight distributions to determine the kinetics of peroxide-induced degradation of polypropylene [J].
Iedema, PD ;
Willems, C ;
van Vliet, G ;
Bunge, W ;
Mutsers, SMP ;
Hoefsloot, HCJ .
CHEMICAL ENGINEERING SCIENCE, 2001, 56 (12) :3659-3669
[9]   Improvement of the mechanical properties of photo-oxidized films after recycling [J].
La Mantia, FP ;
Gardette, JL .
POLYMER DEGRADATION AND STABILITY, 2002, 75 (01) :1-7
[10]   Continuous distribution kinetics for oxidative degradation of PMMA in solution [J].
Madras, G ;
Karmore, V .
POLYMER DEGRADATION AND STABILITY, 2001, 72 (03) :537-541