The effect of diamond-like carbon coatings on the rolling fatigue and wear of M50 steel

被引:49
作者
Rosado, L
Jain, VK [1 ]
Trivedi, HK
机构
[1] Univ Dayton, Dept Mech & Aerosp Engn, Dayton, OH 45469 USA
[2] USAF, Wright Lab, Aero Propuls & Power Directorate, Wright Patterson AFB, OH 45433 USA
[3] Universal Energy Syst Inc, Dayton, OH 45432 USA
关键词
hard coatings; diamond-like carbon; wear; rolling contact fatigue; M50; steel;
D O I
10.1016/S0043-1648(97)00147-6
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The rolling contact fatigue and wear characteristics of uncoated and diamond-like carbon coated VIM-VAR M50 bearing steel were investigated at room temperature and 177 degrees C (350 degrees F) and a Hertzian stress level of 4.8 GPa (700 ksi). The coatings were deposited via ion beam enhanced deposition and were approximately 33 nm thick. Rolling fatigue and wear tests were conducted using a ball-on-rod type tester. Results did not indicate any significant difference in the fatigue rife of coated and uncoated specimens at room temperature, at 90% confidence level. However, the coating significantly improved the fatigue life (90% confidence level) at 177 degrees C and wear resistance at both temperatures. Some correlation was noted between wear and fatigue life for the uncoated specimens at both temperatures, but none for the diamond-like carbon coated (the fatigue life was independent of wear) specimens. Scanning electron microscopy did not show any sign of coating delamination. (C) 1997 Elsevier Science S.A.
引用
收藏
页码:1 / 6
页数:6
相关论文
共 20 条
[11]  
Glover D., 1982, ROLLING CONTACT FATI, P107
[12]  
HIRVONEN J, 1989, WRDCTR894119
[13]   COATINGS TRIBOLOGY - A CONCEPT, CRITICAL ASPECTS AND FUTURE-DIRECTIONS [J].
HOLMBERG, K ;
MATHEWS, A .
THIN SOLID FILMS, 1994, 253 (1-2) :173-178
[14]   SUPERHARD COATINGS FOR METAL-CUTTING APPLICATIONS [J].
INSPEKTOR, A ;
BAUER, CE ;
OLES, EJ .
SURFACE & COATINGS TECHNOLOGY, 1994, 68 :359-368
[15]  
JOHNSON LG, 1964, STAT TREATMENT FATIG, P1
[16]  
KUSTAS FM, 1990, SURF COATING TECHNOL
[17]   ELASTIC-MODULUS OF DIAMOND-LIKE CARBON-FILMS PREPARED BY PULSED VACUUM-ARC [J].
SCHULTRICH, B ;
SCHEIBE, HJ ;
GRANDREMY, G ;
SCHNEIDER, D ;
SIEMROTH, P .
THIN SOLID FILMS, 1994, 253 (1-2) :125-129
[18]  
TRIVEDI HK, 1995, ENG OILS RHEOL TRIB, P83
[19]  
WEI R, 1991, 91TRIB83 ASME
[20]   ROLLING-CONTACT-FATIGUE WEAR CHARACTERISTICS OF DIAMOND-LIKE HYDROCARBON COATINGS ON STEELS [J].
WEI, RH ;
WILBUR, PJ ;
LISTON, MJ ;
LUX, G .
WEAR, 1993, 162 (pt A) :558-568