Hydrophobicity recovery of polydimethylsiloxane after exposure to corona discharges

被引:387
作者
Hillborg, H
Gedde, UW [1 ]
机构
[1] Royal Inst Technol, Dept Polymer Technol, S-10044 Stockholm, Sweden
[2] ABB Corp Res, Dept High Voltage Engn, S-72178 Vasteras, Sweden
关键词
polydimethylsiloxane; hydrophobicity; corona discharges;
D O I
10.1016/S0032-3861(97)00484-9
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A high-temperature-vulcanized polydimethylsiloxane (PDMS) elastomer has been subjected to corona discharges for different periods of time in dry air. The loss and recovery of hydrophobicity of the surface have been characterized by contact angle measurements. Immediately after exposure to corona discharges, samples showed a low surface hydrophobicity and, on storage in dry air, a continuous increase in hydrophobicity finally approaching the hydrophobicity of the unexposed material. The activation energy of the hydrophobicity recovery was two to four times greater than the activation energy of the diffusivity of low molar mass PDMS in PDMS elastomers, indicating that the diffusivity properties of the oxidized surface layer were different from that of the bulk. PDMS elastomers quenched in liquid nitrogen or subjected to small mechanical deformation (<1% strain) after exposure to corona discharges for 1 h or more recovered their hydrophobicity faster than untouched specimens kept under identical conditions. X-ray photoelectron spectroscopy confirmed the early formation of a silica-like surface layer, with a thickness of at least 10-12 nm. The atomic composition of the oxidized surface layer remained essentially unchanged after the first hour of corona discharges. It is suggested that the silica-like surface layer delayed the recovery of hydrophobicity by inhibiting the transport of low molar mass PDMS to the surface. It is also suggested that thermally or purely mechanically induced stresses lead to a cracking of the brittle silica-rich layer and that this in turn facilitates the transport of low molar mass PDMS to the surface and to a more rapid recovery of the hydrophobicity. Data obtained by reflection infrared spectroscopy assessing the outermost micrometer, confirmed the oxidation and the formation of hydroxyl groups at a progressively higher concentration with increasing exposure time of corona discharges. (C) 1998 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1991 / 1998
页数:8
相关论文
共 31 条
  • [11] CONTAMINATION PERFORMANCE OF SILICONE-RUBBER CABLE TERMINATIONS
    GORUR, RS
    JOHNSON, LA
    HERVIG, HC
    [J]. IEEE TRANSACTIONS ON POWER DELIVERY, 1991, 6 (04) : 1366 - 1373
  • [12] HYDROXYLATION OF POLYMETHYLSILOXANE SURFACES BY OXIDIZING PLASMAS
    HOLLAHAN, JR
    CARLSON, GL
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 1970, 14 (10) : 2499 - &
  • [13] HUMMEL D, 1968, ATLAS KUNSTOTOFF ANA, V1
  • [14] KIM SH, 1994, IEEE T DIELECT EL IN, V1, P106, DOI 10.1109/94.300238
  • [15] THE LOSS AND RECOVERY OF HYDROPHOBICITY OF RTV SILICONE-RUBBER INSULATOR COATINGS
    KIM, SH
    CHERNEY, EA
    HACKAM, R
    [J]. IEEE TRANSACTIONS ON POWER DELIVERY, 1990, 5 (03) : 1491 - 1500
  • [16] SUPPRESSION MECHANISM OF LEAKAGE CURRENT ON RTV COATED PORCELAIN AND SILICONE-RUBBER INSULATORS
    KIM, SH
    CHERNEY, EA
    HACKAM, R
    [J]. IEEE TRANSACTIONS ON POWER DELIVERY, 1991, 6 (04) : 1549 - 1556
  • [17] KIM SH, 1992, CONFERENCE RECORD OF THE 1992 IEEE INTERNATIONAL SYMPOSIUM ON ELECTRICAL INSULATION, P237, DOI 10.1109/ELINSL.1992.247012
  • [18] Koenig J.L., 1992, SPECTROSCOPY POLYM, V1st
  • [19] Liang X. D., 1992, Sixth International Conference on Dielectric Materials, Measurements and Applications (Conf. Publ. No.363), P142
  • [20] ON THE AGING OF OXYGEN PLASMA-TREATED POLYDIMETHYLSILOXANE SURFACES
    MORRA, M
    OCCHIELLO, E
    MAROLA, R
    GARBASSI, F
    HUMPHREY, P
    JOHNSON, D
    [J]. JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1990, 137 (01) : 11 - 24