High remnant polarization in (Sr0.7Bi0.2)TiO3-(Na0.5Bi0.5)TiO3 solid solutions

被引:86
作者
Ang, Chen [1 ,2 ]
Yu, Zhi [1 ]
机构
[1] Univ Akron, Dept Phys, Akron, OH 44325 USA
[2] Univ Akron, Dept Chem, Akron, OH 44325 USA
关键词
SINGLE-CRYSTALS; ELECTROSTRICTIVE STRAIN; PHASE-TRANSITIONS; CERAMICS; RELAXOR; NA0.5BI0.5TIO3; DIELECTRICS; BEHAVIOR;
D O I
10.1063/1.3271180
中图分类号
O59 [应用物理学];
学科分类号
摘要
The dielectric and ferroelectric properties of (1-z) (Sr0.7Bi0.2)TiO3-z(Na0.5Bi0.5)TiO3 solid solutions with z=0.65-1 are studied. High remnant polarization of similar to 51 mu C/cm(2) with a coercive field of 50 kV/cm, and a dielectric constant of similar to 1000 have been obtained at room temperature in the sample with z=0.9, indicating an application potential as a lead-free ferroelectric material. There are two dielectric anomalies in the temperature range of 150-670 K for all samples; one is the dielectric peak without significant frequency dispersion, and the other is significantly frequency dependent. The result of this work shows that the formula scheme "a ferroelectric relaxor+a ferroelectric" for solid solutions is a promising approach in the search for high performance lead-free ferroelectric materials. (C) 2009 American Institute of Physics. [doi: 10.1063/1.3271180]
引用
收藏
页数:3
相关论文
共 21 条
[1]   High, purely electrostrictive strain in lead-free dielectrics [J].
Ang, C ;
Yu, Z .
ADVANCED MATERIALS, 2006, 18 (01) :103-106
[2]   Dielectric relaxor and ferroelectric relaxor:: Bi-doped paraelectric SrTiO3 [J].
Ang, C ;
Yu, Z .
JOURNAL OF APPLIED PHYSICS, 2002, 91 (03) :1487-1494
[3]   Intrinsic piezoelectric response in perovskite alloys: PMN-PT versus PZT [J].
Bellaiche, L ;
Vanderbilt, D .
PHYSICAL REVIEW LETTERS, 1999, 83 (07) :1347-1350
[4]   Universal phase diagram for high-piezoelectric perovskite systems [J].
Cox, DE ;
Noheda, B ;
Shirane, G ;
Uesu, Y ;
Fujishiro, K ;
Yamada, Y .
APPLIED PHYSICS LETTERS, 2001, 79 (03) :400-402
[5]   FATIGUE-FREE FERROELECTRIC CAPACITORS WITH PLATINUM-ELECTRODES [J].
DEARAUJO, CAP ;
CUCHIARO, JD ;
MCMILLAN, LD ;
SCOTT, MC ;
SCOTT, JF .
NATURE, 1995, 374 (6523) :627-629
[6]   Reinvestigation of phase transitions in Na0.5Bi0.5TiO3 by TEM.: Part I:: First order rhombohedral to orthorhombic phase transition [J].
Dorcet, V. ;
Trolliard, G. ;
Boullay, P. .
CHEMISTRY OF MATERIALS, 2008, 20 (15) :5061-5073
[7]  
FU F, 2000, NATURE, V403, P281
[8]   Ferroelectric ceramics: History and technology [J].
Haertling, GH .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (04) :797-818
[9]  
Jaffe B., 1971, Piezoelectric Ceramics
[10]   COMPOSITIONAL MODIFICATIONS OF 10-PERCENT-PB-DOPED BI0.5NA0.5TIO3 FOR HIGH-TEMPERATURE DIELECTRICS [J].
KUHARUANGRONG, S ;
SCHULZE, W .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (08) :2274-2278