Properties of mesoporous tungstosilicic acid/titania composites prepared by sol-gel method

被引:13
作者
Blanco, Mirta N. [1 ]
Pizzio, Luis R. [1 ]
机构
[1] UNLP CCT La Plata, CONICET, Ctr Invest & Desarrollo Ciencias Aplicadas Dr JJ, Dept Quim,Fac Ciencias Exactas, RA-1900 La Plata, Argentina
关键词
Titania; Tungstosilicic acid; Urea template; Mesoporous solid; PHOTOCATALYTIC ACTIVITY; TITANIUM-DIOXIDE; TUNGSTOPHOSPHORIC ACID; TUNGSTEN-OXIDE; TIO2; DEGRADATION; PHOTOACTIVITY; HYDROLYSIS; PESTICIDE; SILICA;
D O I
10.1016/j.apsusc.2009.12.105
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The tungstosilicic acid/titania composites were prepared by the sol-gel method. Titanium isopropoxide was used as titania precursor, and urea as a low-cost template. The tungstosilicic acid (TSA) was added in the same step as that in which titania hydrogel is formed. The TSA-modified samples only showed the characteristic peaks of anatase phase of titanium oxide in the XRD patterns, indicating that the presence of TSA retarded the crystallization of the anatase phase and its transformation into the rutile phase. Spherical particles with sizes between 200 and 700 nm, formed by aggregation of nanoparticle aggregates (4-50 nm in size), were observed. The particle size increased when the TSA content was raised and also increased slightly with the thermal treatment temperature. Mesoporous materials were obtained, with a mean pore diameter higher than 3.1 nm. Both the increase of the TSA concentration in the solid and the calcination temperature led to a decrease in the specific surface area of the samples. The main heteropolyoxometallate species present in the composites is the [SiW12O40](4+) anion for the composites calcined up to 500 degrees C. The band gap energy decreased as a result of the introduction of TSA into the titania matrix, though it remained almost constant with the calcination temperature increase. (C) 2010 Elsevier B. V. All rights reserved.
引用
收藏
页码:3546 / 3553
页数:8
相关论文
共 48 条
[21]   Comprehensive evolved gas analysis (EGA) of amorphous precursors for S-doped titania by in situ TG-FTIR and TG/DTA-MS in air: Part 2. Precursor from thiourea and titanium(IV)-n-butoxide [J].
Madarasz, Janos ;
Braileanu, Ana ;
Crisan, Maria ;
Pokol, Gyoergy .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2009, 85 (1-2) :549-556
[22]   OH surface density of SiO2 and TiO2 by thermogravimetric analysis [J].
Mueller, R ;
Kammler, HK ;
Wegner, K ;
Pratsinis, SE .
LANGMUIR, 2003, 19 (01) :160-165
[23]   PHOTO-ADSORPTION AND PHOTO-DESORPTION OF OXYGEN ON HIGHLY HYDROXYLATED TIO2 SURFACES .1. ROLE OF HYDROXYL-GROUPS IN PHOTO-ADSORPTION [J].
MUNUERA, G ;
RIVESARNAU, V ;
SAUCEDO, A .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS I, 1979, 75 :736-747
[24]   PHOTOCATALYTIC DEGRADATION OF CHLOROPHENOLS TO CO2 AND HCL WITH POLYOXOTUNGSTATES IN AQUEOUS-SOLUTION [J].
MYLONAS, A ;
PAPACONSTANTINOU, E .
JOURNAL OF MOLECULAR CATALYSIS, 1994, 92 (03) :261-267
[25]   ESTIMATION OF THE POINT OF ZERO CHARGE OF SIMPLE OXIDES BY MASS TITRATION [J].
NOH, JS ;
SCHWARZ, JA .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1989, 130 (01) :157-164
[26]  
OKUHARA T, 1996, ADV CATAL, V41, P221, DOI DOI 10.1016/S0167-2991(06)80982-1
[27]   Crystallinity effect in the textural properties of titania-TPA catalysts [J].
Ortiz-Islas, E ;
Lopez, T ;
Gomez, R ;
Picquart, M ;
Aguilar, DH ;
Quintana, P .
APPLIED SURFACE SCIENCE, 2005, 252 (03) :853-857
[28]   Investigation of the photocatalytic activity of TiO2-polyoxometalate systems [J].
Ozer, RR ;
Ferry, JL .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2001, 35 (15) :3242-3246
[29]   PHOTOCHEMISTRY OF POLYOXOMETALLATES OF MOLYBDENUM AND TUNGSTEN AND-OR VANADIUM [J].
PAPACONSTANTINOU, E .
CHEMICAL SOCIETY REVIEWS, 1989, 18 (01) :1-31