Indentation fracture behavior of (Mo0.85Nb0.15)Si2 crystals with C40 single-phase and MOSi2(C11b)/NbSi2(C40) duplex-phase with oriented lamellae

被引:18
作者
Hagihara, K
Maeda, S
Nakano, T
Umakoshi, Y
机构
[1] Osaka Univ, Dept Mat Sci & Engn, Grad Sch Engn, Suita, Osaka 5650871, Japan
[2] Osaka Univ, Grad Sch Engn, Handai Frontier Res Ctr, Suita, Osaka 5650871, Japan
关键词
mechanical property; silicide fracture toughness; micro-Vickers hardness test;
D O I
10.1016/j.stam.2003.09.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fracture behavior and toughness of C40-structured (Mo0.85Nb0.15)Si-2 single crystals and MoSi2(C11(b))/NbSi2(C40) duplex-phase crystals with oriented lamellae were investigated by micro-Vickers hardness tests. The indentation fracture toughness in the C40 single-phase showed low values of about 1.0-1.4 MPa m(1/2), while fracture toughness was improved in the duplex-phase crystals. Ductile phase toughening by the C11(b) phase, deflection of crack-propagation at the lamellar boundary and the effect of residual stress field at the crack tip are considered to be responsible for the increment of fracture toughness of MoSi2(C11(b))/NbSi2(C40) duplex-phase crystals. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:11 / 17
页数:7
相关论文
共 19 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]   APPLICATION OF TERNARY PHASE-DIAGRAMS TO THE DEVELOPMENT OF MOSI2-BASED MATERIALS [J].
BOETTINGER, WJ ;
PEREPEZKO, JH ;
FRANKWICZ, PS .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 155 (1-2) :33-44
[3]   Elastic properties of C40 transition metal disilicides [J].
Chu, F ;
Lei, M ;
Maloy, SA ;
Petrovic, JJ ;
Mitchell, TE .
ACTA MATERIALIA, 1996, 44 (08) :3035-3048
[4]   Stacking faults on (001) and their influence on the deformation and fracture behavior of single crystals of MoSi2-WSi2 solid-solutions with the C11b structure [J].
Inui, H ;
Ito, K ;
Nakamoto, T ;
Ishikawa, K ;
Yamaguchi, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 314 (1-2) :31-38
[5]   PLASTIC-DEFORMATION OF MOSI2 SINGLE-CRYSTALS [J].
ITO, K ;
INUI, H ;
SHIRAI, Y ;
YAMAGUCHI, M .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1995, 72 (04) :1075-1097
[6]   MODE OF CHIPPING FRACTURE IN BRITTLE SOLIDS [J].
LAWN, BR ;
SWAIN, MV ;
PHILLIPS, K .
JOURNAL OF MATERIALS SCIENCE, 1975, 10 (07) :1236-1239
[7]   Microstructure and high-temperature strength in MoSi2/NbSi2 duplex silicides [J].
Nakano, T ;
Azuma, M ;
Umakoshi, Y .
INTERMETALLICS, 1998, 6 (7-8) :715-722
[8]   Effect of substitutational elements on plastic deformation behaviour of NbSi2-based silicide single crystals with C40 structure [J].
Nakano, T ;
Kishimoto, M ;
Furuta, D ;
Umakoshi, Y .
ACTA MATERIALIA, 2000, 48 (13) :3465-3475
[9]   Tensile deformation and fracture behaviour in NbSi2 and MoSi2 single crystals [J].
Nakano, T ;
Azuma, M ;
Umakoshi, Y .
ACTA MATERIALIA, 2002, 50 (14) :3731-3742
[10]   Microstructure of duplex-phase NbSi2(C40)/MoSi2(C11b) crystals containing a single set of lamellae [J].
Nakano, T ;
Nakai, Y ;
Maeda, S ;
Umakoshi, Y .
ACTA MATERIALIA, 2002, 50 (07) :1781-1795