Li-ion battery; anode; nitride; Fe doping and degradation mechanism; LITHIUM BATTERIES; ALLOY ANODES; COMPOSITES; ELECTRODES; LI3-XCOXN; NITRIDE; TIN; NI;
D O I
10.1016/S0167-2738(02)00747-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Graphite has been widely used as the anode material of commercial Li-ion secondary battery. With the growing demands of high-capacity secondary battery, the low capacity of graphite (theoretical capacity: 372 mA h/g) has been thought,to be the limiting factor in wide applications and a new anode material with a high capacity has been sought. Of the many materials, Li2.6Co0.4N showed the best anode performance. It showed very high capacity of 1024 mA h/g, good rate capability, (1C/ 0.2C=94.94%) and extraordinary initial coulometric efficiency (96%). In addition to the excellent capacity of this material, its rate capability was much superior to that of graphite (82-88%). However, it cannot be commercialized because its capacity loss after 30 cycles is around 40%.,As a result of various analyses, it was confirmed that the formation of passivating surface film caused by the decomposition reaction between electrolyte and Li2.6Co0.4N is the main reason of its cyclic degradation. As a method of improving the cyclic degradation, iron doping in Li2.6Co0.4N was suggested and we attempted to restrain the formation of passivating film on the surface of Li2.6Co0.4N. Li2.6Co0.35Fe0.05N had a bit lower capacity (about 900 mA h/g) than Li2.6Co0.4N (1024 mA h/g) but showed much better cycle life than Li2.6Co0.4N (35% 60% after 50 cycles). (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:263 / 273
页数:11
相关论文
共 21 条
  • [1] LITHIUM ELECTRODE CYCLEABILITY AND MORPHOLOGY DEPENDENCE ON CURRENT-DENSITY
    ARAKAWA, M
    TOBISHIMA, S
    NEMOTO, Y
    ICHIMURA, M
    YAMAKI, J
    [J]. JOURNAL OF POWER SOURCES, 1993, 43 (1-3) : 27 - 35
  • [2] Will advanced lithium-alloy anodes have a chance in lithium-ion batteries?
    Besenhard, JO
    Yang, J
    Winter, M
    [J]. JOURNAL OF POWER SOURCES, 1997, 68 (01) : 87 - 90
  • [3] Electrochemical and in situ x-ray diffraction studies of the reaction of lithium with tin oxide composites
    Courtney, IA
    Dahn, JR
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (06) : 2045 - 2052
  • [4] STRUCTURE AND ELECTROCHEMISTRY OF LITHIUM COBALT OXIDE SYNTHESIZED AT 400-DEGREES-C
    GUMMOW, RJ
    THACKERAY, MM
    DAVID, WIF
    HULL, S
    [J]. MATERIALS RESEARCH BULLETIN, 1992, 27 (03) : 327 - 337
  • [5] IMPROVED CAPACITY RETENTION IN RECHARGEABLE 4V LITHIUM LITHIUM MANGANESE OXIDE (SPINEL) CELLS
    GUMMOW, RJ
    DEKOCK, A
    THACKERAY, MM
    [J]. SOLID STATE IONICS, 1994, 69 (01) : 59 - 67
  • [6] New amorphous oxides as high capacity negative electrodes for lithium batteries:: the LixMVO4 (M = Ni, Co, Cd, Zn; 1<x≤8) series
    Guyomard, D
    Sigala, C
    La Salle, ALG
    Piffard, SY
    [J]. JOURNAL OF POWER SOURCES, 1997, 68 (02) : 692 - 697
  • [7] Dissolution of spinel oxides and capacity losses in 4V Li/LixMn2O4 coils
    Jang, DH
    Shin, YJ
    Oh, SM
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (07) : 2204 - 2211
  • [8] Electrochemical oxidation processes on Ni electrodes in propylene carbonate containing various electrolyte salts
    Kanamura, K
    Toriyama, S
    Shiraishi, S
    Takehara, Z
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (08) : 2548 - 2558
  • [9] The deterioration behavior of a metal hydride electrode based on the V0.66Ti0.22Ni0.12 alloy
    Kim, JW
    Lee, SM
    Lee, HI
    Kim, DM
    Lee, JY
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 255 (1-2) : 248 - 252
  • [10] Macdonal J.R., 1987, IMPEDANCE SPECTROSCO