Assessment of dielectric behavior of recycled/virgin high density polyethylene blends

被引:11
作者
Cruz, SA [1 ]
Zanin, M [1 ]
机构
[1] UFSCar, DEMa, Dept Mat Engn, BR-13565905 Sao Carlos, SP, Brazil
关键词
recycling; post-consumer; polyethylene; dielectric properties; dielectric strength; volumetric resistivity; stress tracking;
D O I
10.1109/TDEI.2004.1349791
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
In this work, high density polyethylene (HDPE) incorporation in virgin resin was assessed as to its electrical performance with the use of volumetric resistivity, dielectric strength, and stress tracking measurements. HDPE post-consumer packaging was collected and submitted to a basic process of plastic recovering: washing, grinding, and drying. Formulations containing 0, 25, 50, 75, and 100% of recycled material in the virgin resin were reprocessed by extrusion and injection molding with stabilization. Dielectric strength test results were analyzed by the statistical distribution of Weibull, and the maximum likelihood method. The degree of crystallinity was measured by X-ray diffraction. Atomic absorption spectroscopy was also done to identify metallic residue present in the samples. From the results analyzed, it can be concluded that the HDPE derived from post-consumer packaging can be considered in electrical insulation systems for low voltage (up to 600 V) containing as much as 75% incorporated virgin resin.
引用
收藏
页码:855 / 860
页数:6
相关论文
共 19 条
[1]  
CLABBURN RJ, 1972, IEEE T POWER AP SYST, VPA91, P2261
[2]   THE EFFECT OF ALUMINUM INCLUSIONS ON THE DIELECTRIC-BREAKDOWN OF POLYETHYLENE [J].
COPPARD, RW ;
BOWMAN, J ;
DISSADO, LA ;
ROWLAND, SM ;
RAKOWSKI, RT .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1990, 23 (12) :1554-1561
[3]   Dielectric strength of the blends of virgin and recycled HDPE [J].
Cruz, SA ;
Zanin, M .
JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 91 (03) :1730-1735
[4]   Evaluation and identification of degradative processes in post-consumer recycled high-density polyethylene [J].
Cruz, SA ;
Zanin, M .
POLYMER DEGRADATION AND STABILITY, 2003, 80 (01) :31-37
[5]  
Ehrig RJ, 1992, PLASTICS RECYCLING P, P289
[6]   DIELECTRIC-BREAKDOWN PROCESS OF POLYMERS [J].
IEDA, M .
IEEE TRANSACTIONS ON ELECTRICAL INSULATION, 1980, 15 (03) :206-224
[7]   THE INFLUENCE OF MORPHOLOGY ON THE ELECTRIC STRENGTH OF POLYMER INSULATION [J].
KOLESOV, SN .
IEEE TRANSACTIONS ON ELECTRICAL INSULATION, 1980, 15 (05) :382-388
[8]  
Ku CC, 1987, ELECTRICAL PROPERTIE, P102
[9]  
Mancini S. D., 2000, PLASTICO IND, V2, P118
[10]  
Manrich S., 1999, Patent UM, Patent No. 7901580