Fracture toughness of nanocrystalline ZrO2-3mol% Y2O3 determined by vickers indentation

被引:112
作者
Cottom, BA
Mayo, MJ
机构
[1] Dept. of Mat. Sci. and Engineering, Pennsylvania State University, University Park
关键词
D O I
10.1016/1359-6462(95)00587-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
[No abstract available]
引用
收藏
页码:809 / 814
页数:6
相关论文
共 14 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]  
CIFTCIOGLU MH, 1990, MATER RES SOC SYMP P, V196, P77, DOI 10.1557/PROC-196-77
[3]   STUDY OF THE Y-TZP TOUGHNESS BY AN INDENTATION METHOD [J].
GLANDUS, JC ;
ROUXEL, T ;
QIU, T .
CERAMICS INTERNATIONAL, 1991, 17 (02) :129-135
[4]  
GREEN DJ, 1988, TRANSFORMATION TOUGH
[5]   GRAIN-GROWTH IN NANOCRYSTALLINE TIO2 AND ITS RELATION TO VICKERS HARDNESS AND FRACTURE-TOUGHNESS [J].
HOFLER, HJ ;
AVERBACK, RS .
SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (12) :2401-2406
[6]   LATTICE-PARAMETERS AND DENSITY FOR Y2O3-STABILIZED ZRO2 [J].
INGEL, RP ;
LEWIS, D .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1986, 69 (04) :325-332
[7]   INDENTATION STUDIES ON Y2O3-STABILIZED ZRO2 .1. DEVELOPMENT OF INDENTATION-INDUCED CRACKS [J].
KALISZEWSKI, MS ;
BEHRENS, G ;
HEUER, AH ;
SHAW, MC ;
MARSHALL, DB ;
DRANSMANN, GW ;
STEINBRECH, RW ;
PAJARES, A ;
GUIBERTEAU, F ;
CUMBRERA, FL ;
DOMINGUEZRODRIGUEZ, A .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (05) :1185-1193
[8]   CERAMICS DUCTILE AT LOW-TEMPERATURE [J].
KARCH, J ;
BIRRINGER, R ;
GLEITER, H .
NATURE, 1987, 330 (6148) :556-558
[9]   NANOCRYSTALLINE CERAMICS - POSSIBLE CANDIDATES FOR NET-SHAPE FORMING [J].
KARCH, J ;
BIRRINGER, R .
CERAMICS INTERNATIONAL, 1990, 16 (05) :291-294
[10]  
KLUG HP, 1974, XRAY PROCEDURES POLY