Development of new class of ion conductive polymers based on ionic liquids

被引:289
作者
Ohno, H [1 ]
Yoshizawa, M [1 ]
Ogihara, W [1 ]
机构
[1] Tokyo Univ Agr & Technol, Dept Biotechnol, Koganei, Tokyo 1848588, Japan
关键词
ionic liquids; imidazolium salts; polymer electrolytes; ionic conductivity; glass transition temperature;
D O I
10.1016/j.electacta.2004.01.091
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
A series of polymerizable ionic liquid was synthesized and polymerized to prepare new type polymer electrolytes. The effects of position of imidazolium cation, spacer structure and length, and anion species on the ionic conductivity have been investigated. Polycation-type ionic liquids having flexible long spacer showed the ionic conductivity of about 10(-4) S cm(-1) at room temperature. Polyanion-type ionic liquids without spacer structure also showed about 10(-4) S cm(-1) at room temperature. Both examples strongly suggested that the freedom of imidazolium cation affected greatly on the ionic conductivity. Both systems maintained quite low glass transition temperature of about -60degreesC after polymerization. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:255 / 261
页数:7
相关论文
共 41 条
[21]   Bronsted acid-base ionic liquids as proton-conducting nonaqueous electrolytes [J].
Noda, A ;
Susan, AB ;
Kudo, K ;
Mitsushima, S ;
Hayamizu, K ;
Watanabe, M .
JOURNAL OF PHYSICAL CHEMISTRY B, 2003, 107 (17) :4024-4033
[22]   TEMPERATURE-CONTROLLED IONIC-CONDUCTIVITY SWITCHING IN POLY[OLIGO(OXYETHYLENE) METHACRYLATE] POLY(ETHYLENE OXIDE) LAYERED FILM [J].
OHNO, H ;
INOUE, Y ;
WANG, P .
SOLID STATE IONICS, 1993, 62 (3-4) :257-264
[23]   Molten salt type polymer electrolytes [J].
Ohno, H .
ELECTROCHIMICA ACTA, 2001, 46 (10-11) :1407-1411
[24]  
Ohno H, 1998, CHEM LETT, V751
[25]   The performance and stability of ambient temperature molten salts for solar cell applications [J].
Papageorgiou, N ;
Athanassov, Y ;
Armand, M ;
Bonhote, P ;
Pettersson, H ;
Azam, A ;
Gratzel, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (10) :3099-3108
[26]  
Seddon KR, 1997, J CHEM TECHNOL BIOT, V68, P351, DOI 10.1002/(SICI)1097-4660(199704)68:4<351::AID-JCTB613>3.0.CO
[27]  
2-4
[28]   Acid-organic base swollen polymer membranes [J].
Sun, JZ ;
Jordan, LR ;
Forsyth, M ;
MacFarlane, DR .
ELECTROCHIMICA ACTA, 2001, 46 (10-11) :1703-1708
[29]   Characterization of a proton conductor based on silicotungstic acid [J].
Sun, JZ ;
MacFarlane, DR ;
Forsyth, M .
ELECTROCHIMICA ACTA, 2001, 46 (10-11) :1673-1678
[30]  
SUSAN ABH, 2003, CHEM COMMUN, V938