Characterization of Fe-ZSM-5 catalyst for selective catalytic reduction of nitric oxide by ammonia

被引:206
作者
Long, RQ [1 ]
Yang, RT [1 ]
机构
[1] Univ Michigan, Dept Chem Engn, Ann Arbor, MI 48109 USA
关键词
selective catalytic reduction; SCR of NO with ammonia; Fe-exchanged ZSM-5 catalyst; characterization of Fe-ZSM-5; nitrogen oxides;
D O I
10.1006/jcat.2000.2935
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Fe-exchanged ZSM-5 (Fe/Al = 0.193), the most active catalyst known for the selective catalytic reduction (SCR) of NO with ammonia, was characterized by X-ray photoelectron spectroscopy (XPS), H-2 temperature-programmed reduction (H-2-TPR), electron spin resonance (ESR), and FT-IR spectroscopy. XPS and ESR results indicated that iron cations were present mainly as Fe3+ ions with tetrahedral coordination, along with a small amount of Fe2+ and aggregated Fe3+ ions. The Fe3+ ions could be partially reduced to Fe2+ ions by H-2 at 300-600 degrees C, but the oxidation was reversible when O-2 was introduced into the reduced catalyst at 500 degrees C. FTIR spectra showed that NO molecules could be oxidized by O-2 to adsorbed N2O3, NO2, and nitrate. The NOx adspecies were not stable at above 300 degrees C in He, but the adsorbed NO and NO2 could be observed in flowing NO + O-2/He. NH3 molecules were adsorbed on Bronsted acid and Lewis acid sites of Fe-ZSM-5 to generate, respectively, NH4+ ions (majority) and coordinated NH3 (minority). The NH4+ ions with three hydrogen atoms (3H structure) bonded to AlO4 tetrahedra of ZSM-5 were more stable at high temperatures (e.g., 300-400 degrees C) than those with two bonds and the coordinated NH3. The pretreatment by SO2 + O-2 at 400 degrees C increased the Bronsted acidity of the Fe-ZSM-5 due to formation of surface sulfate species of iron. This resulted in an enhancement of SCR activities by the presence of H2O + SO2 at high temperatures (>350 degrees C). At 300 degrees C, the NH4+ ions with 3H structure were active in reacting with NO and NO + O-2, but the reaction rate with NO + O-2 was much higher than that with NO. The results indicate that NH4+ ions with 3H structure as well as NO and NO2 adspecies play an important role in the SCR reaction on the Fe-ZSM-5 catalyst. The role of Fe3+ is to oxidize NO to NO2. Overexchange decreased the activity; the optimal Fe/Al ratio was 0.19-0.43. (C) 2000 Academic Press.
引用
收藏
页码:80 / 90
页数:11
相关论文
共 46 条
[11]   SPECTROSCOPIC CHARACTERIZATION OF THE FE/ZRO2 SYSTEM .2. NO ADSORPTION AND CO-NO REACTION [J].
GUGLIELMINOTTI, E .
JOURNAL OF PHYSICAL CHEMISTRY, 1994, 98 (36) :9033-9038
[12]   Problems in preparation of FeZSM-5 catalysts [J].
Hall, WK ;
Feng, XB ;
Dumesic, J ;
Watwe, R .
CATALYSIS LETTERS, 1998, 52 (1-2) :13-19
[13]   FRAMEWORK HYDROXYL-GROUPS OF H-ZSM-5 ZEOLITES [J].
JACOBS, PA ;
VONBALLMOOS, R .
JOURNAL OF PHYSICAL CHEMISTRY, 1982, 86 (15) :3050-3052
[14]   MECHANISM OF THE REACTION OF NITRIC-OXIDE, AMMONIA, AND OXYGEN OVER VANADIA CATALYSTS .1. THE ROLE OF OXYGEN STUDIED BY WAY OF ISOTOPIC TRANSIENTS UNDER DILUTE CONDITIONS [J].
JANSSEN, FJJG ;
VANDENKERKHOF, FMG ;
BOSCH, H ;
ROSS, JRH .
JOURNAL OF PHYSICAL CHEMISTRY, 1987, 91 (23) :5921-5927
[15]   Preparation, characterization, and performance of Fe-ZSM-5 catalysts [J].
Joyner, R ;
Stockenhuber, M .
JOURNAL OF PHYSICAL CHEMISTRY B, 1999, 103 (29) :5963-5976
[16]  
KATO A, 1981, J PHYS CHEM-US, V85, P4099, DOI 10.1021/j150626a029
[17]   In situ high-temperature ESR characterization of FeZSM-5 and FeSAPO-34 catalysts in flowing mixtures of NO, C3H6, and O2 [J].
Kucherov, AV ;
Montreuil, CN ;
Kucherova, TN ;
Shelef, M .
CATALYSIS LETTERS, 1998, 56 (04) :173-181
[18]  
Laane J., 1980, Prog Inorg Chem, V27, P465, DOI [10.1002/9780470166284.ch6, DOI 10.1002/9780470166284.CH6]
[19]   SELECTIVE REDUCTION OF NOX BY METHANE ON CO-FERRIERITES .2. CATALYST CHARACTERIZATION [J].
LI, YJ ;
SLAGER, TL ;
ARMOR, JN .
JOURNAL OF CATALYSIS, 1994, 150 (02) :388-399
[20]   An in situ infrared study of NO reduction by C3H8 over Fe-ZSM-5 [J].
Lobree, LJ ;
Hwang, IC ;
Reimer, JA ;
Bell, AT .
CATALYSIS LETTERS, 1999, 63 (3-4) :233-240