SOME POSSIBILITIES FOR IMPROVING THE HOLOGRAPHIC RECORDING CHARACTERISTICS IN BI12SIO20 MONOCRYSTALS

被引:6
作者
MITEVA, MG
机构
关键词
D O I
10.1109/JQE.1986.1073113
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
引用
收藏
页码:1365 / 1368
页数:4
相关论文
共 16 条
[1]  
Gudaev O. A., 1978, Avtometriya, P92
[2]  
Gusev V. A., 1983, Avtometriya, P34
[3]   NANOSECOND 4-WAVE MIXING AND HOLOGRAPHY IN BSO CRYSTALS [J].
HERMANN, JP ;
HERRIAU, JP ;
HUIGNARD, JP .
APPLIED OPTICS, 1981, 20 (13) :2173-2175
[4]  
HUIGNARD JP, 1979, OPT LETT, V4, P21, DOI 10.1364/OL.4.000021
[5]   HIGH-SENSITIVITY READ-WRITE VOLUME HOLOGRAPHIC STORAGE IN BI12SIO20 AND BI12GEO20 CRYSTALS [J].
HUIGNARD, JP ;
MICHERON, F .
APPLIED PHYSICS LETTERS, 1976, 29 (09) :591-593
[6]   REAL-TIME DOUBLE-EXPOSURE INTERFEROMETRY WITH BI12SIO20 CRYSTALS IN TRANSVERSE ELECTROOPTIC CONFIGURATION [J].
HUIGNARD, JP ;
HERRIAU, JP .
APPLIED OPTICS, 1977, 16 (07) :1807-1809
[7]   EFFECT OF INFRARED IRRADIATION ON HOLOGRAPHIC RECORDING IN BISMUTH SILICON-OXIDE [J].
KAMSHILIN, AA ;
MITEVA, MG .
OPTICS COMMUNICATIONS, 1981, 36 (06) :429-433
[8]  
KAMSHILIN AA, 1982, Patent No. 34999
[9]  
LEONHARDT K, 1983, OPTIK, V65, P33