THICKNESS SWELLING AND DENSITY VARIATION IN ASPEN FLAKEBOARDS

被引:11
作者
LIU, JY
MCNATT, JD
机构
[1] USDA Forest Service Forest Products Laboratory, Madison, 53705-2398, WI, One Gifford Pinchot Drive
关键词
D O I
10.1007/BF00195558
中图分类号
S7 [林业];
学科分类号
0829 ; 0907 ;
摘要
This paper reports the relationship between thickness swelling and density in labmade aspen flakeboards. The boards were manufactured with several levels of initial mat moisture content and urea resin content. Weight increase and thickness swelling at 12 locations on each board were recorded under specified environmental conditions over a period of 71 days. Each board was then cut into 12 specimens, each containing one of the 12 locations at its center, and density was calculated. No definite relationship was found between thickness swelling and density among the 12 specimens of each board. Our results suggest that high initial moisture content and high resin content can decrease thickness swelling. Variations in mat pressure and core temperature during the press cycle and weight increase at 80 percent relative humidity are discussed. © 1991 Springer-Verlag.
引用
收藏
页码:73 / 82
页数:10
相关论文
共 17 条
[11]  
Maku T., 1959, WOOD RES, V21, P34
[12]  
Stewart H. A., 1973, Forest Products Journal, V23, P52
[13]  
Strickler M. D., 1959, Forest Products Journal, V9, P203
[14]  
Suchsland O., 1959, Quarterly Bulletin. Michigan State University Agricultural Experiment Station, V42, P350
[15]  
SUCHSLAND O, 1967, FOREST PROD J, V17, P51
[16]  
SUCHSLAND O., 1973, FOREST PROD J, V23, P26
[17]  
TOMIMURA Y, 1986, MOKUZAI GAKKAISHI, V32, P170