摘要
Recent work has shown that under carefully controlled conditions secondary ring-opening reactions can be avoided to give a clean modification of NR with any desired level of epoxidation. For the sake of simplicity, three grades of epoxidized NR are discussed: ENR-50 with 50 mole% epoxidation, ENR-25 with 25 mole% epoxidation, and ENR-10 with 10 mole% epoxidation. Substantial physical property changes occur with the extend of epoxidation, and the special features of the new rubbers are described.
引用
收藏
页码:67 / 85
页数:19
相关论文
共 16 条
  • [1] BAKER CSL, 1983, KAUT GUMMI KUNSTST, V36, P677
  • [2] BARNARD D, 1975, P INT RUBBER C
  • [3] BLOOMFIELD GF, 1934, J SOC CHEM IND LOND, V53, pT121
  • [4] CAIN ME, 1972, RUBBER CHEM TECHNOL, V45, P204
  • [5] CAMPBELL DS, 1981, KAUTSCH GUMMI KUNSTS, V34, P636
  • [6] STRAIN CRYSTALLIZATION IN RANDOM CO-POLYMERS PRODUCED BY EPOXIDATION OF CIS 1,4-POLYISOPRENE
    DAVIES, CKL
    WOLFE, SV
    GELLING, IR
    THOMAS, AG
    [J]. POLYMER, 1983, 24 (01) : 107 - 113
  • [7] DAWES K, 1978, PLAST RUBBER MATER A, V3, P23
  • [8] MODIFICATION OF NATURAL-RUBBER LATEX WITH PERACETIC-ACID
    GELLING, IR
    [J]. RUBBER CHEMISTRY AND TECHNOLOGY, 1985, 58 (01): : 86 - 96
  • [9] GELLING IR, 1985, RUBBER CHEM TECHNOL, V58
  • [10] GONSOVSKAYA TB, 1971, KAUCH REZINA, V30, P23