EFFECTS OF IMPURITIES AND SUPPORTING ELECTROLYTES ON SCC OF 304 STAINLESS-STEEL IN HIGH-TEMPERATURE AQUEOUS ENVIRONMENTS

被引:19
作者
ANDRESEN, PL [1 ]
INDIG, ME [1 ]
机构
[1] GE,VALLECITOS NUCL CTR,PLEASANTON,CA 94566
关键词
421 Strength of Building Materials; Mechanical Properties - 539 Metals Corrosion and Protection; Metal Plating - 545 Iron and Steel;
D O I
10.5006/1.3593856
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
AS-WELDED, LOW TEMPERATURE SENSITIZED AND FURNACE SENSITIZED 304 HAS BEEN STUDIED UNDER TWO CONDITIONS OF POTENTIAL CONTROL: VARIABLE ADDITIONS OF OXYGEN AND HYDROGEN PEROXIDE IN PURE AND IMPURE WATER AND POTENTIOSTAT IN DEAERATED SUPPORTING ELECTROLYTE. IMPURITY ADDITIONS AND TRANSIENT TEMPERATURETESTING ACCELERATE INTERGRANULAR STRESS CORROSION CRACKING.TESTING IN SUPPORTING ELECTROLYTES OFTEN YIELDS MISLEADING RESULTS.
引用
收藏
页码:531 / 541
页数:11
相关论文
共 41 条
[1]  
ANDRESEN P, UNPUB
[2]   THE EFFECTS OF DISSOLVED-OXYGEN, CHLORIDE-ION AND APPLIED POTENTIAL ON THE SCC BEHAVIOR OF TYPE-304 STAINLESS-STEEL IN 290-DEGREES-C WATER [J].
ANDRESEN, PA ;
DUQUETTE, DJ .
CORROSION, 1980, 36 (08) :409-415
[3]  
ANDRESEN PA, 1979, THESIS RENSSELAER PO
[4]   CRACK INITIATION IN CERT TESTS ON TYPE-304 STAINLESS-STEEL IN PURE WATER [J].
ANDRESEN, PL .
CORROSION, 1982, 38 (01) :53-59
[5]   EFFECT OF CHLORIDE-ION CONCENTRATION AND APPLIED POTENTIAL ON THE SCC BEHAVIOR OF TYPE-304 STAINLESS-STEEL IN DE-AERATED HIGH-TEMPERATURE WATER [J].
ANDRESEN, PL ;
DUQUETTE, DJ .
CORROSION, 1980, 36 (02) :85-93
[6]  
ANDRESEN PL, 1981, INVESTIGATION BENEFI
[7]  
ASAY RH, 1980, WATER QUALITY BOILIN
[8]   ELECTRONIC PROPERTIES OF OXIDE-FILMS AND PITTING SUSCEPTIBILITY OF TPE-304 STAINLESS-STEEL [J].
BIANCHI, G ;
CERQUETTI, A ;
TORCHIO, S ;
MAZZA, F .
CORROSION SCIENCE, 1972, 12 (06) :495-+
[9]  
CRANGNOLINO G, 1981, CORROSION, V37, P312
[10]  
DANIELSON MJ, 1979, CORROSION, V35, P201