THE INFLUENCE OF AGING AT 180-DEGREES-C ON THE CORROSION BEHAVIOR OF A TERNARY AL-LI-ZR ALLOY

被引:4
作者
AMBAT, R
PRASAD, RK
DWARAKADASA, ES
机构
[1] Department of Metallurgy, Indian Institute of Science, Bangalore
关键词
D O I
10.1016/0010-938X(95)00030-N
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of aging at 180 degrees C on the corrosion behaviour of an Al-1.5%Li-0.1%Zr alloy has been studied using weight loss, open circuit potential (OCP) measurements and potentiodynamic polarization measurements in 3.5% NaCl solution. Corrosion rates obtained from weight loss and I-corr values decreased for samples aged up to 6 h at 180 degrees C whereas I-corr increased for samples aged for longer times. Values of OCP and pitting potential initially shifted in the noble direction and then towards more active values. This change in OCP was observed on samples that had been aged for 20 h while in the case of pitting potential an aging time of only 6 h was required. The overall change in passive current density was small, although at longer aging times (> 40h) it showed an increase. As the amount of lithium depletion increased, OCP and pitting potential shifted in the active direction while passive current density showed an increase. The results have been interpreted in terms of the microstructure.
引用
收藏
页码:1253 / 1265
页数:13
相关论文
共 37 条
[21]  
SANDERS TH, 1980, MATER SCI ENG, V43, P260
[22]  
SANDERS TH, 1979, FINAL REPORT NAVAL A
[23]   THE STRUCTURE AND PROPERTIES OF SPLAT-QUENCHED ALUMINUM-ALLOY 2024 CONTAINING LITHIUM ADDITIONS [J].
SANKARAN, KK ;
GRANT, NJ .
MATERIALS SCIENCE AND ENGINEERING, 1980, 44 (02) :213-227
[24]  
SANKARAN KK, 1992, CORROS SCI, V33, P205
[25]  
SATER JM, 1989, 5TH P INT AL LITH C, V3, P1217
[26]   MICROSTRUCTURAL CHARACTERIZATION OF 2 LITHIUM-CONTAINING ALUMINUM-ALLOYS [J].
SRIVATSAN, TS ;
COYNE, EJ ;
STARKE, EA .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (05) :1553-1560
[27]  
STARKE EA, 1986, 1ST P INT C AL ALL
[28]  
STARKE EA, 1983, 2ND P INT C AL LITH
[29]  
STARKE EA, 1981, 1ST P INT C AL LITH, P1
[30]   SURFACE DEPLETION OF LITHIUM IN MEDIUM-STRENGTH AERONAUTICAL AL-LI ALLOYS DURING HEAT-TREATMENT [J].
UDYAVAR, MS ;
DWARAKADASA, ES .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1992, 11 (08) :490-492