THE TOUGHNESS OF EPOXY-POLY(BUTYLENE TEREPHTHALATE) BLENDS

被引:26
作者
NICHOLS, ME [1 ]
ROBERTSON, RE [1 ]
机构
[1] UNIV MICHIGAN,DEPT MAT SCI & ENGN,ANN ARBOR,MI 48109
关键词
D O I
10.1007/BF00366876
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Blends containing 5% poly(butylene terephthalate) (PBT) in an anhydride-cured epoxy with three different PBT morphologies were studied. The three morphologies were a dispersion of spherulites, a structureless gel and a gel with spherulites. The average fracture toughnesses, K-lc and fracture energies, G(lc) for those morphologies were 0.83, 2.3 and 1.8 MPam(1/2) and 240, 2000 and 1150 Jm(-2), respectively. These values should be compared with the values of 0.72 MPam(1/2) and 180 Jm(-2), respectively, for the cured epoxy without PBT. The elastic moduli and yield strengths in compression for all three blend morphologies remained essentially unchanged from those of the cured epoxy without PBT, namely, 2.9 GPa for the modulus and 115 MPa for the yield strength, The fracture surfaces of the cured spherulitic dispersion blends indicate the absorption of fracture energy by crack bifurcation induced by the spherulites. The fracture surfaces of the cured structureless gel blends indicate that fracture energy was absorbed by matrix and PBT plastic deformation and by spontaneous crack bifurcation. But phase transformation of the PBT and anelastic strain of the matrix below the fracture surfaces may account for most of the large fracture energy of the cured structureless gel blends.
引用
收藏
页码:5916 / 5926
页数:11
相关论文
共 56 条
[52]   PHASE-STRUCTURE AND ADHESION IN POLYMER BLENDS - A CRITERION FOR RUBBER TOUGHENING [J].
WU, SH .
POLYMER, 1985, 26 (12) :1855-1863
[53]   THE SYNTHESIS AND MORPHOLOGY OF SEMI-INTERPENETRATING POLYMER NETWORKS BASED ON POLYURETHANE POLYDIMETHYLSILOXANE SYSTEM [J].
XIAO, H ;
PING, ZH ;
XIE, JW ;
YU, TY .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1990, 28 (03) :585-594
[54]  
YEE AF, 1986, J MATER SCI, V21, P2462, DOI 10.1007/BF01114293
[55]   STRUCTURES OF 2 CRYSTALLINE FORMS OF POLY(BUTYLENE TEREPHTHALATE) AND REVERSIBLE TRANSITION BETWEEN THEM BY MECHANICAL DEFORMATION [J].
YOKOUCHI, M ;
SAKAKIBARA, Y ;
CHATANI, Y ;
TADOKORO, H ;
TANAKA, T ;
YODA, K .
MACROMOLECULES, 1976, 9 (02) :266-273
[56]   FAILURE OF BRITTLE POLYMERS BY SLOW CRACK GROWTH .3. EFFECT OF COMPOSITION UPON FRACTURE OF SILICA PARTICLE-FILLED EPOXY-RESIN COMPOSITES [J].
YOUNG, RJ ;
BEAUMONT, PWR .
JOURNAL OF MATERIALS SCIENCE, 1977, 12 (04) :684-692