POLYMORPHISM IN SYNDIOTACTIC POLYSTYRENE - A H-1-NMR RELAXATION STUDY

被引:52
作者
CAPITANI, D
DEROSA, C
FERRANDO, A
GRASSI, A
SEGRE, AL
机构
[1] CNR,IST STRUTTURIST CHIM G GIACOMELLO,MB 10,MONTEROTONDO STN,I-00016 ROME,ITALY
[2] MONTEDIPE SPA,I-46100 MANTOVA,ITALY
[3] SALERNO UNIV,DEPT PHYS,I-84081 SALERNO,ITALY
[4] NAPLES UNIV,DEPT CHEM,I-80134 NAPLES,ITALY
关键词
D O I
10.1021/ma00041a008
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A marked shortening of T, relaxations in solid aromatic polymers can be attributed to O2 adsorbed on the aromatic rings. This effect, observed as a function of temperature, is modulated by the amount of adsorbed O2, Which, in turn, varies according to the molecular packing and crystalline/amorphous ratio. Within the temperature range 77-400 K, semicrystalline syndiotactic polystyrenes (s-PS) in the alpha, beta, and gamma-polymorph modifications were studied by pulse H-1 NMR at 30 MHz. Due to the presence of many relaxation components, 1,2,2-trideuterio-s-PS was synthesized, crystallized, and characterized by X-ray powder diffraction. At low temperature, when both the O2 diffusion and the spin-diffusion processes are slow enough, the backbone-deuteriated polymers exhibit multiple T1 relaxations: three for alpha and beta s-PS and two for gamma s-PS. These T1 components are attributed to crystalline and amorphous phases. From the study of these components as a function of temperature and from direct comparison of T1 values in the different phases, the following conclusions were drawn: (i) Clear differentiation was possible between different s-PS polymorphs. (ii) Determination of the crystalline vs amorphous ratio fully consistent with X-ray diffraction data was achieved. (iii) The amorphous component of different semicrystalline s-PS polymorphs could be distinguished.
引用
收藏
页码:3874 / 3880
页数:7
相关论文
共 35 条
[21]   AN ALGORITHM FOR LEAST-SQUARES ESTIMATION OF NONLINEAR PARAMETERS [J].
MARQUARDT, DW .
JOURNAL OF THE SOCIETY FOR INDUSTRIAL AND APPLIED MATHEMATICS, 1963, 11 (02) :431-441
[22]  
MICHALKO VK, 1984, ZH STRUKT KHIM, V25, P3
[23]   STRUCTURE OF THE AMORPHOUS PHASE IN CRYSTALLIZABLE POLYMERS - POLY(ETHYLENE-TEREPHTHALATE) [J].
MURTHY, NS ;
CORREALE, ST ;
MINOR, H .
MACROMOLECULES, 1991, 24 (05) :1185-1189
[24]  
PELLECCHIA C, 1987, MAKROMOL CHEM-RAPID, V8, P277
[25]  
PERSICO M, IN PRESS AB INITIO C
[26]   LOCAL AND COOPERATIVE MOTIONS AT THE GLASS-TRANSITION OF POLYSTYRENE - INFORMATION FROM ONE-DIMENSIONAL AND 2-DIMENSIONAL NMR AS COMPARED WITH OTHER TECHNIQUES [J].
PSCHORN, U ;
ROSSLER, E ;
SILLESCU, H ;
KAUFMANN, S ;
SCHAEFER, D ;
SPIESS, HW .
MACROMOLECULES, 1991, 24 (02) :398-402
[27]  
RAPACCIUOLO M, IN PRESS J MATER SCI
[28]  
SEGRE AG, IN PRESS
[29]  
SEGRE AL, 1986, POLYM COMMUN, V27, P216
[30]  
SYKORA S, PROGRAM FIT PART SOF