SUPERPLASTIC BEHAVIOR OF A FINE-GRAINED, YTTRIA-STABILIZED, TETRAGONAL ZIRCONIA POLYCRYSTAL (Y-TZP)

被引:172
作者
NIEH, TG
WADSWORTH, J
机构
[1] Lockheed Missiles and Space Company, Inc., Research and Development Division, O-9310, B-204, 3251 Hanover Street, Palo Alto
来源
ACTA METALLURGICA ET MATERIALIA | 1990年 / 38卷 / 06期
关键词
Activation Energy - Flow Stress - Grain Growth - High Temperature Properties - Strain Rate - Yttria Stabilized Tetragonal Zirconia Polycrystals;
D O I
10.1016/0956-7151(90)90185-J
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and deformation characteristics of a fine-grained superelastic yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) have been investigated. Both hot indentation and tensile tests were carried out at temperatures between 1273 and 1923K over the strain rate range from 2.7 × 10-5 to 2 × 10-3 s-1. It was found that the material exhibited extensive plasticity at temperatures higher than 1473K; a maximum tensile elongation of over 800% was recorded. Microstructural examination did not indicate the presence of a glassy phase at grain boundaries. Yttrium, however, was found to segregate to the grain boundaries. The microstructure of the Y-TZP was thermally unstable and appreciable grain growth was observed at emperattures higher than 1723 K; the grain growth was enhanced by external stresses, i.e. dynamic grain growth was observed. Grain growth at elevated temperatures resulted in apparent strain rate sensitivity exponents of approximately 0.33 at 1723K. This value decreased with increasing temperature. The grain size-compensated strain rate, however, was found to depend approximately on the square of the flow stress, i.e. to exhibit a true strain sensitivity value of 0.5, which suggests a grain boundary sliding mechanism. Microstructures from samples that were deformed superelastically indicated that grains remained equiaxed; this observation is consistent with a grain boundary sliding mechanism. The activation energy for superplasticity, under the conditions of constant structure, in Y-TZP was calculated to be 720 kJ/mol. © 1990.
引用
收藏
页码:1121 / 1133
页数:13
相关论文
共 58 条
[31]   SUPERPLASTIC BEHAVIOR OF A 20-PERCENT AL2O3/YTZ CERAMIC COMPOSITE [J].
NIEH, TG ;
MCNALLY, CM ;
WADSWORTH, J .
SCRIPTA METALLURGICA, 1989, 23 (04) :457-460
[32]   SUPERPLASTIC PROPERTIES OF A FINE-GRAINED YTTRIA-STABILIZED TETRAGONAL POLYCRYSTAL OF ZIRCONIA [J].
NIEH, TG ;
MCNALLY, CM ;
WADSWORTH, J .
SCRIPTA METALLURGICA, 1988, 22 (08) :1297-1300
[33]  
NIEH TG, 1989, IN PRESS J AM CERAM
[34]  
NIEH TG, 1989, IMAM7 SUPERPLASTICIT, P251
[35]  
OISHI Y, 1983, ADDITIVES INTERFACES, V7, P208
[36]  
OKAMOTO Y, 1988, ADV CERAM, V24, P565
[37]   ON CREEP ENHANCED BY A LIQUID-PHASE [J].
PHARR, GM ;
ASHBY, MF .
ACTA METALLURGICA, 1983, 31 (01) :129-138
[38]   MEASUREMENTS OF SUPERPLASTICITY IN AN AL-CU ALLOY [J].
RAI, G ;
GRANT, NJ .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1975, 6 (02) :385-390
[39]   ENHANCED DENSIFICATION OF WHITE CAST-IRON POWDERS BY CYCLIC PHASE-TRANSFORMATIONS UNDER STRESS [J].
RUANO, OA ;
WADSWORTH, J ;
SHERBY, OD .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (03) :355-361
[40]   HIGH-TEMPERATURE CREEP OF Y2O3-STABILIZED ZRO2 [J].
SELTZER, MS ;
TALTY, PK .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1975, 58 (3-4) :124-130