SM2FE17-NITRIDE-BASED PERMANENT-MAGNETS PRODUCED BY THE HYDROGENATION DECOMPOSITION DESORPTION RECOMBINATION (HDDR) PROCESS

被引:55
作者
CHRISTODOULOU, CN
TAKESHITA, T
机构
[1] Central Research Institute, Mitsubishi Materials Corporation, Omiya, Saitama, 330
关键词
D O I
10.1016/0925-8388(93)90587-D
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The hydrogenation-decomposition-desorption-recombination (HDDR) process in conjunction with nitrogenation has been employed to produce Sm2Fe17-nitride-based permanent magnets. The HDDR process has been studied in terms of the reaction characteristics, the phases present and the development of the magnetic properties at the different stages involved in the process. On heating under hydrogen gas, the Sm2Fe17 phase begins to absorb hydrogen at a temperature of about 185-degrees-C and up to 250-degrees-C, where the hydrogen concentration reaches a maximum value of about 2.4 H atoms per mole of Sm2Fe17. Subsequently, interstitial hydrogen desorption occurs gradually up to a temperature of 510-degrees-C (SM2Fe17H0.1), where a massive absorption of hydrogen takes place owing to the decomposition of the Sm2Fe17H0.1 into Sm hydride + alpha-Fe. Additional beat treatment of the ''Sm hydride + alpha-Fe'' mixture at temperatures of about 725-degrees-C or above under vacuum or argon gas flow causes the simultaneous desorption of the Sm hydride (forming Sm + H-2) and recombination of Sm + alpha-Fe to form microcrystalline grains of the Sm2Fe17 phase. Subsequent nitrogenation at about 450-degrees-C produces Sm2Fe17-nitride which exhibits an intrinsic coercivity of 8.2 kOe, a Curie temperature of 470-degrees-C and a maximum energy product of about 14 MG Oe.
引用
收藏
页码:155 / 159
页数:5
相关论文
共 22 条
[11]  
COEY JMD, 1990, 6TH P INT S MAGN AN, P36
[12]   SM2(FE,M)17NX COMPOUNDS AND MAGNETS [J].
ENDOH, M ;
IWATA, M ;
TOKUNAGA, M .
JOURNAL OF APPLIED PHYSICS, 1991, 70 (10) :6030-6032
[13]   METAL-BONDED SM2FE17-N-TYPE MAGNETS [J].
HUANG, MQ ;
ZHANG, LY ;
MA, BM ;
ZHENG, Y ;
ELBICKI, JM ;
WALLACE, WE ;
SANKAR, SG .
JOURNAL OF APPLIED PHYSICS, 1991, 70 (10) :6027-6029
[14]   MAGNETISM OF (SM,R)2FE17NY (R=Y, TB OR MISCHMETAL) [J].
HUANG, MQ ;
ZHENG, Y ;
MILLER, K ;
ELBICKI, JM ;
SANKAR, SG ;
WALLACE, WE .
JOURNAL OF APPLIED PHYSICS, 1991, 70 (10) :6024-6026
[15]  
HUANG MQ, 1990, 6TH P INT S MAGN AN, P204
[16]   STRUCTURAL AND MAGNETIC-PROPERTIES OF THE RARE-EARTH IRON NITRIDE SOLUTION SERIES Y2(FE1-XCOX)17N3-DELTA [J].
HURLEY, DPF ;
COEY, JMD .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1991, 99 (1-3) :229-234
[17]   STRUCTURAL AND HARD MAGNETIC-PROPERTIES OF RAPIDLY SOLIDIFIED SM-FE-N [J].
KATTER, M ;
WECKER, J ;
SCHULTZ, L .
JOURNAL OF APPLIED PHYSICS, 1991, 70 (06) :3188-3196
[18]   KERR MICROSCOPY OBSERVATION OF NITROGENATED SM2FE17 INTERMETALLIC COMPOUNDS [J].
MUKAI, T ;
FUJIMOTO, T .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1992, 103 (1-2) :165-173
[19]  
NAKAMURA H, 1991, 15TH ANN C MAGN JAP, P379
[20]   HIGH COERCIVITY IN SM2FE17NX MAGNETS [J].
SCHNITZKE, K ;
SCHULTZ, L ;
WECKER, J ;
KATTER, M .
APPLIED PHYSICS LETTERS, 1990, 57 (26) :2853-2855