EFFECT OF HEAT-TREATMENT ON DELAYED HYDRIDE CRACKING IN ZR-2.5 WT PCT NB

被引:26
作者
AMOUZOUVI, KF
CLEGG, LJ
机构
来源
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1987年 / 18卷 / 10期
关键词
D O I
10.1007/BF02646200
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:1687 / 1694
页数:8
相关论文
共 30 条
[1]   AGE HARDENING OF ZR-2.5 WT PERCENT NB SLOWLY COOLED FROM (ALPHA+BETA) PHASE FIELD [J].
ALDRIDGE, SA ;
CHEADLE, BA .
JOURNAL OF NUCLEAR MATERIALS, 1972, 42 (01) :32-&
[2]  
AMBLER JF, 1985, AECL PRFM73P AT EN C
[3]  
AMOUZOUVI KF, 1986, UNPUB
[4]  
BIRNBAUM HK, 1976, SCRIPTA METALL MATER, V10, P747, DOI 10.1016/0036-9748(76)90355-0
[5]  
BIRNBAUM HK, 1974, HYDROGEN METALS, P303
[6]   METALLOGRAPHIC STUDY OF THE TERMINAL SOLUBILITY OF HYDROGEN IN ZIRCONIUM AT LOW HYDROGEN CONCENTRATIONS [J].
CANN, CD ;
ATRENS, A .
JOURNAL OF NUCLEAR MATERIALS, 1980, 88 (01) :42-50
[7]   SOLUBILITY OF HYDROGEN ISOTOPES IN STRESSED HYDRIDE-FORMING METALS [J].
COLEMAN, CE ;
AMBLER, JFR .
SCRIPTA METALLURGICA, 1983, 17 (01) :77-82
[8]  
COLEMAN CE, 1978, CAN MET Q, V17, P81
[9]  
COLEMAN CE, 1977, ASTM STP, V633, P589
[10]   MECHANISMS OF HYDROGEN INDUCED DELAYED CRACKING IN HYDRIDE FORMING MATERIALS [J].
DUTTON, R ;
NUTTALL, K ;
PULS, MP ;
SIMPSON, LA .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1977, 8 (10) :1553-1562