CONDITIONS FOR COMPLETE SELF-HEALING BREAKDOWN IN GLOW-DISCHARGE POLYMERIZED STYRENE FILMS

被引:11
作者
SAWA, G [1 ]
ARAKAWA, K [1 ]
NAGAO, M [1 ]
IEDA, M [1 ]
机构
[1] NAGOYA UNIV, DEPT ELECT ENGN, NAGOYA, AICHI 464, JAPAN
关键词
D O I
10.1016/0040-6090(79)90286-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Breakdown patterns of glow discharge polymerized styrene film sandwiched between the top and base electrodes and fabricated on a glass substrate have been observed with a microscope. The breakdown patterns can be classified into three types: a broad ring of partly vanishing top electrode metal occuring around the breakdown hole in the dielectric (type A); a large hole made through the three layers (one dielectric and two metal layers), the dielectric film and the top electrode being folded back together at the periphery of the hole and the base electrode being melted over the hole area (type B); successive breakdown around the periphery of previous breakdown spots (type P). These patterns are interpreted in terms of the action of an arc across an extremely short gap as well as joule heating. Type A is preferable for attaining complete self-healing and the conditions that most favour the occurrence of type A holes are (a) the application of a positive voltage to the top electrode and (b) the top electrode being thin compared with the base electrode. © 1979.
引用
收藏
页码:131 / 141
页数:11
相关论文
共 19 条