Influence of surface modification of fillers and polymer on flammability and tensile behaviour of polypropylene-composites

被引:66
作者
Demir, H [1 ]
Balköse, D [1 ]
Ülkü, S [1 ]
机构
[1] Fac Engn, Izmir Inst Technol, Dept Chem Engn, TR-35430 Izmir, Turkey
关键词
natural zeolite; mechanical properties; flame retardant-polypropylene; intumescent; coupling agent; polypropylene;
D O I
10.1016/j.polymdegradstab.2005.07.012
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
An intumescent system consisting of ammonium polyphosphate (APP) as an acid source and blowing agent, pentaerythritol (PER) as a carbonific agent and natural zeolite (clinoptilolite, Gordes II) as a synergistic agent was used in this study to enhance flame retardancy of polypropylene (FR-PP). Zeolite was incorporated into flame retardant formulation at four different concentrations (1, 2, 5, and 10 wt%) to investigate synergism with the flame retardant materials. Filler content was fixed at 30 wt% of total amounts of flame retardant PP composites. Zeolite and APP were treated with two different coupling agents namely, 3-(trimethoxysityl)-1-propanethiol and (3-aminopropyl)-triethoxysilane for investigation of the influence of surface treatments on mechanical properties and flame retardant performance of composites. Maleic anhydride grafted polypropylene (MAPP) was used for making polypropylene hydrophilic. Flammability of FR-PP composites was measured by the determination of limiting oxygen index (LOI). The LOI values reached to a maximum value of 41% for mercapto silane treated APP:PER (2:1) PP composite containing 5 wt% zeolite. The tensile strength of composites was increased by the addition of MAPP and elongation at break of composites was increased with silane treatments. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1079 / 1085
页数:7
相关论文
共 20 条
[1]   Intumescent flame retardant systems of modified rheology [J].
Anna, P ;
Marosi, G ;
Bourbigot, S ;
Le Bras, M ;
Delobel, R .
POLYMER DEGRADATION AND STABILITY, 2002, 77 (02) :243-247
[2]  
*ASTM, 1991, 286391 ASTM D
[3]   Role of interface modification in filled and flame-retarded polymer systems [J].
Bertalan, G ;
Marosi, G ;
Anna, P ;
Ravadits, I ;
Csontos, I ;
Tóth, A .
SOLID STATE IONICS, 2001, 141 :211-215
[4]   Synergistic effect of zeolite in an intumescence process: Study of the carbonaceous structures using solid-state NMR [J].
Bourbigot, S ;
LeBras, M ;
Delobel, R ;
Decressain, R ;
Amoureux, JP .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1996, 92 (01) :149-158
[5]  
BOURBIGOT S, 1996, FIRE MAT, V20
[6]   Synergistic effect of natural zeolites on flame retardant additives [J].
Demir, H ;
Arkis, E ;
Balköse, D ;
Ülkü, S .
POLYMER DEGRADATION AND STABILITY, 2005, 89 (03) :478-483
[7]   Surface modification and adhesion mechanisms in woodfiber-polypropylene composites [J].
Kazayawoko, M ;
Balatinecz, JJ ;
Matuana, LM .
JOURNAL OF MATERIALS SCIENCE, 1999, 34 (24) :6189-6199
[8]   Investigation of mechanical property, flame retardancy and thermal degradation of LLDPE-wood-fibre composites [J].
Li, B ;
He, JM .
POLYMER DEGRADATION AND STABILITY, 2004, 83 (02) :241-246
[9]   Fire retardancy effect of migration in polypropylene nanocomposites induced by modified interlayer [J].
Marosi, G ;
Márton, A ;
Szép, A ;
Csontos, I ;
Keszei, S ;
Zimonyi, E ;
Toth, A ;
Almeras, X .
POLYMER DEGRADATION AND STABILITY, 2003, 82 (02) :379-385
[10]   Modified interfaces in multicomponent polypropylene fibers [J].
Marosi, G ;
Tohl, A ;
Bertalan, G ;
Anna, P ;
Maatoug, MA ;
Ravadits, I ;
Bertoti, I ;
Toth, A .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1998, 29 (9-10) :1305-1311