Smooth fine-grained diamond coatings on titanium alloy for mechanical applications

被引:25
作者
De Barros, MI
Vandenbulcke, L
Chinsky, L
Rats, D
von Stebut, J
机构
[1] CNRS, Lab Combust & Syst Reactifs, F-45071 Orleans 2, France
[2] Univ Paris 06, Lab Physicochim Biomol & Cellulaire, F-75252 Paris 5, France
[3] Ecole Mines Nancy, Lab Sci & Genie Surfaces, F-54042 Nancy, France
关键词
smooth fine-grained diamond; visible and UV Raman spectroscopy; hardness; Young's modulus;
D O I
10.1016/S0925-9635(00)00433-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Smooth, fine-grained diamond coatings have been deposited on titanium alloy by a two-step microwave PACVD process at 600 degreesC. Their morphology and roughness were studied by scanning electron microscopy and atomic force microscopy in comparison with polycrystalline coatings. The diamond purity of all these coatings in terms of sp(3) bonding fraction was deduced from visible and UV Raman spectroscopy as a function of the deposition conditions. Finally, the influence of diamond purity on hardness, Young's modulus and residual stresses of the coatings are reported. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:337 / 341
页数:5
相关论文
共 20 条
[1]  
ABOUELLEIL M, 1990, CERAM T, V15, P457
[2]  
Ager JW, 1995, MATER RES SOC SYMP P, V383, P143, DOI 10.1557/PROC-383-143
[3]   QUANTITATIVE MEASUREMENT OF RESIDUAL BIAXIAL STRESS BY RAMAN-SPECTROSCOPY IN DIAMOND GROWN ON A TI ALLOY BY CHEMICAL-VAPOR-DEPOSITION [J].
AGER, JW ;
DRORY, MD .
PHYSICAL REVIEW B, 1993, 48 (04) :2601-2607
[4]   RAMAN INVESTIGATIONS ON DIAMOND FILMS AND CRYSTALS DEPOSITED BY PLASMA-ASSISTED CVD [J].
BOU, P ;
VANDENBULCKE, L .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1991, 138 (10) :2991-3000
[5]  
BOU P, 1989, P 1 INT S DIAM DIAM, P610
[6]  
Budinski K. G., 1991, ASME, P289
[7]   Plasma-assisted chemical vapor deposition process for depositing smooth diamond coatings on titanium alloys at moderate temperature [J].
De Barros, MI ;
Vandenbulcke, L .
DIAMOND AND RELATED MATERIALS, 2000, 9 (11) :1862-1866
[8]   Tribological performance of diamond-coated Ti-6Al-4V alloy with respect to diamond characteristics [J].
De Barros, MI ;
Vandenbulcke, L ;
Fontaine, J ;
Farges, G ;
Vayer, M ;
Erre, R .
SURFACE & COATINGS TECHNOLOGY, 2000, 127 (2-3) :193-202
[9]   Influence of internal diffusion barriers on carbon diffusion in pure titanium and Ti-6Al-4V during diamond deposition [J].
De Barros, MI ;
Rats, D ;
Vandenbulcke, L ;
Farges, G .
DIAMOND AND RELATED MATERIALS, 1999, 8 (06) :1022-1032
[10]  
DEBARROS MI, UNPUB